LAIRD TGON 805

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

LAIRD TGON 805

Main features

  • 0.13 mm Flexible Graphite Interface
  • 5 W/(m K) Through-Plane Conductivity
  • 0.07 deg C in^2/W Thermal Resistance

Product Description

Laird Tgon™ 805 is the 0.13 mm-thick configuration of the Tgon™ 800 Series, a flexible graphite interface pad designed for applications where electrical isolation is not required and both electrical contact and thermal transfer are desired. Its grain-oriented, plate-like graphite structure provides typical thermal conductivity of 5 W/m·K through the Z axis and 240 W/m·K in the X-Y plane. The material contains more than 98% graphite and is available without adhesive or with a thin pressure-sensitive adhesive on one side to aid assembly.

Key Features

  • 0.13 mm nominal thickness for thin electrically and thermally conductive interfaces.
  • Anisotropic thermal conductivity of 5 W/m·K through-plane and 240 W/m·K in-plane.
  • More than 98% graphite construction with low thermal resistance and optional one-side pressure-sensitive adhesive.

Applications / Suitable for

  • Power conversion equipment
  • Power supplies
  • Large telecommunications switching hardware
  • Notebook computers
  • Applications requiring electrical grounding with thermal conductivity

Technical Specifications

General Properties
Color
Pewter
Component System
Flexible Graphite
Density (g)
2.2 g/cm3
Thickness range
0.13 mm
Thermal Properties
Operating Temperature
-240 to 300 °C
Thermal Conductivity
5 W/m.K
UL 94 Rating
V0
Electrical Properties
Volume Resistivity
11 x 10^-5 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties for the 0.13 mm Tgon™ 805 configuration of the Tgon™ 800 Series.

Property Value Unit Method / condition
Construction Flexible graphite — Typical specification
Color Pewter — Visual
Nominal thickness 0.005 in Equivalent to 0.13 mm
Thickness tolerance ±0.001 in Equivalent to ±0.025 mm
Density 2.20 g/cc Helium pycnometer
Hardness 85 Shore A ASTM D2240
Technical properties

After-processing / final-state properties

Typical installed and in-use properties for Tgon™ 805. Thermal resistance is reported at the stated interface pressure.

Property Value Unit Method / condition
Thermal conductivity, Z axis 5 W/m·K ASTM D5470, modified
Thermal conductivity, X-Y axis 240 W/m·K ASTM D5470, modified
Thermal resistance 0.07 °C·in²/W ASTM D5470, modified; 100 psi
Thermal resistance 0.42 °C·cm²/W ASTM D5470, modified; 681 kPa
Tensile strength 650 psi ASTM D412
Volume resistivity, in-plane 11 × 10−5 ohm·cm ASTM D257
Temperature range −240 to 300 °C Without adhesive; adhesive-backed material is rated 0 to 120°C