LAIRD TFLEX 6110

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

LAIRD TFLEX 6110

Main features

  • 3 W/mK Thermal Conductivity
  • Greater Than 90% Recovery
  • Naturally Tacky Adhesive-Free Placement

Product Description

Tflex 6110 Thermal Gap Filler is a 0.110 inch (2.79 mm) boron-nitride-filled silicone elastomer pad for component-to-hardware thermal gaps. The soft, naturally tacky material combines 3 W/(m K) thermal conductivity with Shore 00 hardness of 25, supporting low-pressure contact without an added adhesive coating. It recovers to more than 90% of its original thickness after compression and remains electrically insulating. Applications include component-to-chassis cooling, storage drives, memory modules, heat-pipe assemblies, automotive control units, and telecommunications hardware.

Key features

  • 3 W/(m K) Conductive Pad: Boron-nitride-filled silicone supports heat transfer across compressed electronic gaps.
  • Greater Than 90% Recovery: The material returns toward its original thickness after low-pressure compression.
  • Naturally Tacky Placement: Surface tack supports installation without an added adhesive coating.

Applications / Suitable for

  • Cooling components to chassis or frames
  • Storage drives, memory modules, and heat-pipe assemblies
  • Automotive control units and telecommunications hardware
Product Family

LAIRD TFLEX 6110

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Blue-Violet
Component System
Ceramic filled silicone sheet
Density (g)
1.34 g/cm3
Thermal Properties
Operating Temperature
(-)45 to 200 °C
Thermal Conductivity
3.0 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical Tflex 600-series construction and mechanical properties for the 0.110 inch Tflex 6110 configuration.

Property Value Unit Method / condition
Construction Boron-nitride-filled silicone elastomer Tflex 600 series
Nominal thickness 0.110 in 2.79 mm Tflex 6110 configuration
Color Blue-violet Visual
Density 1.34 g/cc Helium pycnometer; unreinforced grade
Hardness 25 Shore 00 ASTM D2240
Tensile strength 15 psi ASTM D412
Elongation 75 % ASTM D412
Surface Naturally tacky No additional adhesive coating required
Technical properties

After-processing / final-state properties

Typical Tflex 600-series thermal, recovery, electrical, and outgassing properties; interface resistance depends on thickness and assembly pressure.

Property Value Unit Method / condition
Thermal conductivity 3 W/(m K) Modified ASTM D5470
Thickness recovery Greater than 90 % After low-pressure compression
Operating temperature -45 to 200 deg C Typical series range
Breakdown voltage Greater than 5,000 VAC ASTM D149
Volume resistivity 2 x 10^13 ohm cm ASTM D257
Dielectric constant 3.31 At 1 MHz; ASTM D150
Outgassing TML 0.13 % Post-cured; ASTM E595
Outgassing CVCM 0.05 % Post-cured; ASTM E595