LAIRD MCS/SS6M

Harmonization Code : 3215907090 | Ink, whether or not concentrated or solid (excl. printing ink, printer/copier ink cartridges incorporating mechanical or electrical components, and solid ink in engineered shapes for printers/copiers)

LAIRD MCS/SS6M

Main features

  • 800 MHz to 6 GHz Absorption
  • Low-Outgassing Silicone Construction
  • Flexible Sheet with Optional PSA

Product Description

Laird Eccosorb® MCS is a thin, flexible, magnetically loaded silicone rubber microwave absorber designed for frequencies from 800 MHz to 6 GHz. The electrically non-conductive sheet combines high magnetic loss with moisture resistance, low outgassing and a maximum service temperature of 170°C. It is used to suppress surface currents, creeping waves and cavity resonances, and to reduce RF coupling between antennas and microwave components. The material conforms to contoured surfaces, can be cut with a sharp knife and is available with optional pressure-sensitive adhesive backing.

Key features

  • Broad microwave coverage: Designed for absorption across the 800 MHz to 6 GHz frequency range.
  • Low-outgassing silicone construction: Provides 0.3% TML and 0.05% CVCM when tested according to ASTM E595-07.
  • Flexible installation: Conforms to contoured surfaces and is available with optional pressure-sensitive adhesive backing.

Applications / Suitable for

  • Surface-current and creeping-wave suppression
  • Cavity-resonance reduction in microwave modules
  • Reduction of RF coupling between antennas and microwave components
  • Commercial telecom, defense, automotive and industrial electronics
Product Family

LAIRD MCS/SS6M

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
UL 94 Rating
V0
Mechanical Properties
Elongation
20 %
Electrical Properties
Dielectric Strength
0.78 kV/mm