KESTER 959T Soldering Flux

Harmonization Code : 29051200 | Propan-1-ol (propyl alcohol) and propan-2-ol (isopropyl alcohol)

KESTER 959T Soldering Flux

Main features

  • Excellent wetting
  • Low rosin content
  • Non-corrosive

Product Description

KESTER 959T is a no-clean, non-corrosive liquid flux formulated for wave soldering of both conventional and surface mount circuit board assemblies. Formulated to reduce micro-solderball formation, 959T liquid flux delivers superior soldering performance and cosmetic results.

Product Key Features

  • Excellent wetting for high quality solder joints.
  • Low rosin content (0.5%), improving solderability, heat stability, and and high surface insulation resistance.
  • Non-corrosive
  • Even residue distribution

Applications

  • Wave soldering of conventional through-hole assemblies & surface mount technology (SMT) boards. 
Product Family

KESTER 959T

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 3 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
2.9 %
Specific Gravity
0.794
Thermal Properties
Flash Point
18 °C

Additional Information

Flux Application

959T can be applied to circuit boards by a spray, foam, or dip process. Flux deposition should be 120 to 240ug of solids/cm2 (750 to 1500 ug/in2). An air knife after the flux tank is recommended to remove excess flux from the circuit board and prevent dripping on the preheated surface. 