KESTER 5252 Cleaner

Harmonization Code : 29051200 | Propan-1-ol (propyl alcohol) and propan-2-ol (isopropyl alcohol)

KESTER 5252 Cleaner

Main features

  • Quickly air dries
  • Halogen-free formulation
  • Non-ionic

Product Description

Kester 5252 Cleaner is an environmentally friendly, halogen-free solvent designed for efficient cleaning in electronics manufacturing. 5252 offers rapid air-drying and effective removal of contaminants without ozone depletion.

Product Key Features

  • Non-ozone depleting and safe for the environment.
  • Fast air-drying
  • Rapidly dissolves solder pastes, flux residues, and organic contaminants.
  • Non-ionic & low toxicity
  • Suitable replacement for traditional chlorinated cleaning agents.

Applications

Product Family

KESTER 5252

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
Shipping in 3 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
solubility
100 Min
Specific Gravity
0.788
Thermal Properties
Boiling Point
82 °C
Flash Point
9 °C

Additional Information

Application

5252 can be used as a solvent for the following applications: stencil cleaning, cleaning of misprinted assemblies, removal of post-soldering flux residues and other organic contaminants from electronic assemblies (wave-soldered and reflow processes), and general purpose cleaning.

5252 may be used at ambient temperature with ultrasonics, stencil spray equipment, or immersion agitation or manual application. When the residue has completely dissolved and is no longer visible, the residual solution is rinsed off with more solvent. The purpose is not to only dissolve the residue, but also to remove it after it is dissolved.

5252 dries fast and usually does not require any water rinse. It is recommended that after cleaning with 5252 solvent, the stencils or electronic assemblies should be dried by evaporation or solvent displacement with forced air. If additional cleanliness is required, the stencils or assemblies could be rinsed with a secondary 5252 rinse. The bath life of the cleaner solvent will depend on the cleanliness requirements. The solvent should be replaced at regular intervals in order to avoid solvent contamination.