KESTER 186-18

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

KESTER 186-18

Main features

  • High-Preheat Thermal Stability
  • RMA-Style Flux Activity
  • Low-Corrosion No-Clean Residue

Product Description

Kester 186-18 Mildly Activated Rosin Liquid Flux is a Type RMA-style flux for critical electronic assemblies and multilayer boards that require high preheat stability. Its rosin system approaches activated-rosin fluxing performance while leaving a non-conductive, non-corrosive residue that normally does not require removal. The flux can be applied by foam or dip methods, with a typical board-side preheat range of 90 to 105 deg C. A low-corrosion test profile and IPC SIR pass support controlled use in circuit-board soldering. Applications include difficult circuit-board assemblies, multilayer assemblies, and processes that specify mildly activated rosin flux.

Key features

  • High-Preheat Stability: The flux retains useful processing behavior for multilayer assemblies using 90 to 105 deg C board-side preheat.
  • RMA-Style Flux Activity: Fluxing ability approaches activated rosin while retaining mildly activated residue behavior.
  • Low-Corrosion Residue: Post-solder residue is non-conductive, non-corrosive, and passes IPC SIR testing.

Applications / Suitable for

  • Foam or dip fluxing of circuit boards
  • Critical electronic assemblies
  • Multilayer assemblies with high preheat
Product Family

KESTER 186-18

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
18 %
Specific Gravity
0.831 typical @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid-flux properties and storage limits before soldering.

Property Value Unit Method / condition
Flux classification ROL0 / ROL1 IPC J-STD-004 / J-STD-004B
Specific gravity 0.831 Typical at 25 deg C
Flash point 18 deg C 64 deg F
Typical solids 18 % As supplied
Board-side preheat 90 to 105 deg C Typical circuit assemblies
Shelf life 2 years Stored at 10 to 25 deg C