KESTER 1544

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

KESTER 1544

Main features

  • Activated Rosin Oxide Removal
  • Fast Wetting and Capillary Flow
  • Non-Conductive Post-Solder Residue

Product Description

Kester 1544 Activated Rosin Liquid Flux is an alcohol-based, activated rosin flux for electronic soldering, solder coating, and tinning. The ROM1 formulation combines 50% typical solids with rapid wetting and capillary flow where non-activated or mildly activated rosin fluxes do not provide enough oxide removal. It can be applied by brush, dip, or wave methods and supports typical board-side preheat temperatures of 90 to 105 deg C. The post-solder residue is non-conductive and non-corrosive and normally does not require removal. Applications include wave soldering, lead tinning, and assembly processes requiring an activated rosin flux.

Key features

  • Activated Rosin Wetting: ROM1 chemistry supports rapid wetting and capillary flow where stronger oxide removal is required.
  • 50% Solids Flux Control: The high-solids rosin formulation is controlled by specific gravity during use.
  • Non-Conductive Residue: Post-solder residue is non-conductive, non-corrosive, and normally left in place.

Applications / Suitable for

  • Electronic assembly wave soldering
  • Solder coating
  • Tinning bare leads
Product Family

KESTER 1544

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
50 %
Specific Gravity
0.917–0.928 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid-flux properties and storage limits before soldering.

Property Value Unit Method / condition
Flux classification ROM1 J-STD-004
Specific gravity 0.917 to 0.928 At 25 deg C
Typical solids 50 % J-STD-004; IPC-TM-650 Method 2.3.34
Flash point 18 deg C 64 deg F
VOC content 459 g/liter As supplied
Chloride and bromides 0.44 % IPC-TM-650 Method 2.3.35
Shelf life 2 years Stored at 10 to 25 deg C