JNC PI-6322-001 | Insulating Polyimide Ink

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

JNC PI-6322-001 | Insulating Polyimide Ink JNC PI-6322-001 | Insulating Polyimide Ink

Main features

  • Thermal Curable
  • Heat Resistance
  • Low Temperature Curing

Product Description

PI-6322-001 is a polyimide insulating ink designed to provide thermally curable solution to heat resistance and electrical insulation. It is engineered to provide electrical insulation with its advanced polyimide formulation ensures that your components remain safeguarded against electrical currents, allowing your devices to perform flawlessly even in high-voltage applications. Featured with only 1% water absorbance, this ink stands strong against moisture-induced vulnerabilities, guaranteeing consistent performance even in humid environments. Moreover, with a tensile modulus of 1500 MPa, this ink enhances mechanical stability, making it an excellent choice for applications requiring both electrical insulation and structural integrity.

Industry Applications:

Aerospace and Defense | Electronics Manufacturing | Industrial Sensors

Product Family

JNC PI-6322-001

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Process Method
Inkjet
Solids
24 %
Thermal Properties
Glass Transition Temperature (Tg)
250 °C
Electrical Properties
Breakdown Voltage
100 V
Volume Resistivity
10000000000000000 Ohms⋅cm
Mechanical Properties
Elongation
6 %
Chemical Properties
Water Absorption
1 %
Physical Properties
Viscosity
11 mPa.s

Additional Information

Properties PI-6322-001
Solids content (wt. %) 24
Viscosity (mPa's) @25℃ 11
Surface tension (mN/m) @23℃ 28
Printing methods Inkjet
Curing 180℃
120min
Post-curing -
Volume resistivity (Ω*cm) 1E+16
Breakdown voltage (V/um) 100
Dielectric constant (1kHz) @1V 3.8
Tensile modulus (MPa) 1500
Elongation (%) 6
Residual stress (MPa) 14
5% weight loss temp (℃) 370
CTE ( 75
Tg (℃) 250
Water absorbance (%) @23℃ 1.0