JNC PA-1210-034 | Insulating Polyacrylate Ink

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

JNC PA-1210-034 | Insulating Polyacrylate Ink JNC PA-1210-034 | Insulating Polyacrylate Ink

Main features

  • UV Curable/ Solvent free
  • High Insulation reliability for fine pitch devices
  • Advance Sensors

Product Description

PA-1210-034 is a UV-curable, solvent-free polyacrylate insulating in, sets a new benchmark for high insulating reliability in fine pitch devices. Its specialized polyacrylate composition offers robust dielectric properties, creating an insulating layer that guarantees the utmost in reliability. Its tensile modulus of 1600 MPa, this ink augments mechanical stability, making it an excellent choice for applications requiring both electrical insulation and structural integrity. Also features a residual stress of 14 MPa and a coefficient of thermal expansion (CTE) of 91 ppm/K, ensuring compatibility with diverse materials and minimizing the risk of performance-altering mismatches.

Industry Applications:

Fine Pitch Electronics | Microfabrication| Advance Sensors

Product Family

JNC PA-1210-034

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Process Method
Inkjet
Solids
100 %
Thermal Properties
Glass Transition Temperature (Tg)
136 °C
Electrical Properties
Breakdown Voltage
80 V
Volume Resistivity
1000000000000000 Ohms⋅cm
Mechanical Properties
Elongation
4 %
Chemical Properties
Water Absorption
0.4 %
Physical Properties
Viscosity
35 mPa.s

Additional Information

Properties PA-1210-034
Solids content (wt. %) 100
Viscosity (mPa's) @25℃ 35
Surface tension (mN/m) @23℃ 31
Printing methods Inkjet
Curing 2,000mJ/cm2
 @ 365nm
Post-curing 175℃
60min
Volume resistivity (Ω*cm) 1E+15
Breakdown voltage (V/um) 80
Dielectric constant (1kHz) @1V 3.1
Tensile modulus (MPa) 1600
Elongation (%) 4
Residual stress (MPa) 14
5% weight loss temp (℃) 295
CTE ( 91
Tg (℃) 136
Water absorbance (%) @23℃ 0.4