JNC PA-1210-020 | Insulating Polyacrylate Ink

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

JNC PA-1210-020 | Insulating Polyacrylate Ink JNC PA-1210-020 | Insulating Polyacrylate Ink

Main features

  • UV Curable/ Solvent free
  • Standard
  • Optoelectronics

Product Description

PA-1210-020 is a UV-curable, solvent-free polyacrylate insulating ink. Its advanced polyacrylate composition ensures robust dielectric properties of a breakdown voltage of 100 V/um and a dielectric constant of 3.2 @ 1 kHz, ensuring dependable electrical isolation and signal integrity for your components. Moreover, with its solvent-free formulation, PA-1210-020 contributes to a safer and more environmentally friendly production process, minimizing volatile organic compounds (VOCs) and reducing the ecological footprint.

 

Industry Applications:

Electronics Manufacturing | Optoelectronics | Microelectronics

Product Family

JNC PA-1210-020

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Process Method
Inkjet
Solids
100 %
Thermal Properties
Glass Transition Temperature (Tg)
116 °C
Electrical Properties
Breakdown Voltage
100 V
Mechanical Properties
Elongation
3 %
Chemical Properties
Water Absorption
0.2 %
Physical Properties
Viscosity
23 mPa.s

Additional Information

Properties PA-1210-020
Solids content (wt. %) 100
Viscosity (mPa's) @25℃ 23
Surface tension (mN/m) @23℃ 30
Printing methods Inkjet
Curing 2,000mJ/cm2
 @ 365nm
Post-curing 175℃
60min
Volume resistivity (Ω*cm) 1E+16
Breakdown voltage (V/um) 100
Dielectric constant (1kHz) @1V 3.2
Tensile modulus (MPa) 1800
Elongation (%) 3
Residual stress (MPa) 12
5% weight loss temp (℃) 275
CTE ( 55
Tg (℃) 116
Water absorbance (%) @23℃ 0.2