FM-DA11 | Reactive PDMS - Monoterminal Hydroxy (Diol)

Harmonization Code : 3910.00.00.60 | Polydimethylsiloxane, whether or not polyethylene glycol and trifluoropropyl substituted, with methacrylate end groups

FM-DA11 | Reactive PDMS - Monoterminal Hydroxy (Diol)

Main features

  • Mono terminal
  • 1,000 g/mol | 60 mPas
  • Hydroxy (Diol) functional group

Product Description

Silaplane® FM-DA11 is a reactive polydimethylsiloxane (PDMS) based polymer with a molecular weight of 1,000 g/mol and a Viscosity of 60 mPas. This reactive silicone material offers the addition of silicone-type properties to non-Silicone materials in a variety of industries including electronics, semiconductors, automotive, biotech, healthcare, and clean energy applications. It offers narrow polydispersity and a low level of chemical impurities

Silaplane® FM-DA11 mono-terminal product has a Hydroxy (Diol) functional group that is reactive toward a variety of compounds and surfaces enabling chemical and physical changes to chemicals, particle surfaces and larger surface structures. Hydroxy groups are mainly reacting with Urethane and Ester compounds. The reactive functional group improves the adsorption to the filler surface and makes the inorganic filler easier to blend into the silicone binder resin. At the same time it displays high affinity for the silicone binder resin which improves the wettability between the filler and the binder. This product stabilizes the filler dispersion due to the repulsive force between fillers, achieved by silicone repulsion and the osmotic pressure effect.

Product Benefits:

  • Filler dispersion stabilization with low viscosity
  • Water/Oil repellency
  • Gas permeability (Oxygen, CO2, CH4, etc.)
  • Mold releasability
  • Anti-Abrasion resistance, Anti-fouling
Product Family

JNC FM-DA11

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Molecular weight
1000 g/mol
Specific Gravity
0.97
Physical Properties
Viscosity
60 mPa.s