INDIUM SMQ92J

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

INDIUM SMQ92J

Main features

  • High-Speed Fine-Pitch Printing
  • Long Stencil and Tack Life
  • Probe-Testable No-Clean Residue

Product Description

Indium NC-SMQ92J No-Clean Solder Paste is a halogen-free, air-reflow solder paste for high-speed surface-mount assembly. The flux system supports consistent fine-pitch deposition, extended open time, strong initial tack, and more than 12 hours of stencil life under the stated conditions. It leaves a benign, probe-testable residue that can be penetrated by multi-point probes without clogging. A typical Sn63 Type 3 printing configuration has 2,000 poise viscosity and 38 g tackiness. Applications include fast-print SMT lines, rapid component placement, fine-pitch printing, and air or nitrogen reflow with the supported SnPb alloy configurations.

Key features

  • High-Speed SMT Printing: Supports fast print speeds and rapid component placement with consistent fine-pitch deposition.
  • Long Stencil and Tack Life: More than 12 hours of stencil life under stated conditions combines with strong initial tack.
  • Probe-Testable Residue: Benign residue is penetrated by multi-point probes without clogging.

Applications / Suitable for

  • High-speed SMT printing
  • Fine-pitch component placement
  • SnPb air or nitrogen reflow
Product Family

INDIUM SMQ92J

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Stencil Life
More than 12 h hours

Additional Information

Technical properties

As-supplied / before-processing properties

Typical pre-reflow values for NC-SMQ92J; the specified Sn63 Type 3 printing configuration is identified where required.

Property Value Unit Method / condition
Flux classification ROL0 J-STD-004
Typical viscosity 2,000 poise Sn63, 90.25% metal load, Type 3; Malcolm at 10 rpm
Typical thixotropic index -0.75 SSF; ICA test
Typical tackiness 38 g J-STD-005 test result
Stencil life greater than 12 hours 30 to 60% RH at 22 to 28 deg C
Shelf life 6 months Unopened container stored below 10 deg C