INDIUM NC-SMQ92H

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

INDIUM NC-SMQ92H

Main features

  • Consistent Fine-Pitch Deposition
  • Extended Stencil and Tack Life
  • Low-Spatter Halogen-Free Reflow

Product Description

Indium NC-SMQ92H No-Clean Solder Paste is a halogen-free, air-reflow solder paste formulated for fine-pitch deposition with low flux spatter. It combines consistent printing, more than 12 hours of stencil life under the stated conditions, and a hard, clear residue after reflow. The ROL0 flux system shows typical tackiness of 32 g and a typical viscosity of 1,400 poise for the specified Sn63 Type 3 configuration. NC-SMQ92H is supplied for both stencil printing and dispensing formats and can be processed in air or nitrogen. Applications include fine-pitch SMT printing, dispensing, and reflow using supported SnPb alloy configurations.

Key features

  • Fine-Pitch Deposition: Consistent printing and a minimum 1.5 aperture aspect ratio support fine-feature stencil release.
  • Extended Stencil Life: Stencil life exceeds 12 hours at 22 to 28 deg C and 30 to 60% RH.
  • Low-Spatter No-Clean Flux: Halogen-free ROL0 flux is formulated for low spatter and air reflow.

Applications / Suitable for

  • Fine-pitch SMT printing
  • Solder paste dispensing
  • SnPb air or nitrogen reflow
Product Family

INDIUM NC-SMQ92H

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Stencil Life
More than 12 h hours

Additional Information

Technical properties

As-supplied / before-processing properties

Typical pre-reflow values for NC-SMQ92H; alloy, metal load, and powder configuration are retained where required.

Property Value Unit Method / condition
Flux classification ROL0 J-STD-004
Typical viscosity 1,400 poise Sn63, 90% metal load, Type 3; Malcolm at 10 rpm
Typical thixotropic index -0.75 SSF; ICA test
Typical tackiness 32 g J-STD-005 test result
Stencil life greater than 12 hours 30 to 60% RH at 22 to 28 deg C
Shelf life 6 months Unopened container stored below 10 deg C