INDIUM 8.9HF1

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

INDIUM 8.9HF1

Main features

  • 0.4 mm CSP Print Transfer
  • Oxidation-Barrier Defect Control
  • Highly Probe-Testable Residue

Product Description

Indium8.9HF1 Pb-Free Solder Paste is a halogen-free, no-clean solder paste for air reflow with SAC305 and supported powder configurations. The flux system provides oxidation control for small deposits, supports print transfer on 0.4 mm pitch CSP apertures, and leaves a highly probe-testable residue for in-circuit testing. A typical SAC305 Type 4 viscosity of 1,300 poise and more than 12 hours of stencil life under the stated shop conditions support controlled SMT printing. The paste is used for lead-free assembly in air or nitrogen reflow. Applications include fine-pitch CSP printing, surface-mount assembly, and reflow processes using the stated SAC alloy configurations.

Key features

  • 0.4 mm CSP Transfer: Supports print transfer efficiency on 0.4 mm pitch CSP features.
  • Oxidation Barrier: Flux chemistry helps suppress graping and head-in-pillow defects.
  • Probe-Testable Residue: The no-clean residue supports in-circuit testing after reflow.

Applications / Suitable for

  • 0.4 mm pitch CSP printing
  • Lead-free surface-mount assembly
  • SAC305 air or nitrogen reflow
Product Family

INDIUM 8.9HF1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Stencil Life
More than 12 h hours

Additional Information

Technical properties

As-supplied / before-processing properties

Typical pre-reflow properties for Indium8.9HF1 with the stated SAC305 powder configuration and handling conditions.

Property Value Unit Method / condition
Flux classification ROL0 IPC J-STD-004D
Typical viscosity 1,300 poise SAC305 Type 4 powder
Metal load 88.50 % SAC305 Type 3 powder
Metal load 88.25 % SAC305 Type 4 powder
Stencil life greater than 12 hours 30 to 60% RH at 22 to 28 deg C
Shelf life 6 months Unopened container stored below 10 deg C