INDIUM 8.9HF

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

INDIUM 8.9HF

Main features

  • Stable Small-Aperture Printing
  • Clear Probe-Testable Residue
  • Low-Voiding High-Temperature Reflow

Product Description

Indium8.9HF Pb-Free Solder Paste is a halogen-free, no-clean solder paste for air reflow in lead-free electronics assembly. The flux system is formulated for stable stencil printing, high transfer efficiency through apertures at or below 0.66 area ratio, and low voiding in BGA, CSP, and QFN joints. It leaves a clear, probe-testable residue and supports long or high-temperature reflow profiles. The paste also wets oxidized BGA and pad surfaces under the stated process conditions. Applications include fine-feature SMT printing and lead-free reflow where the ordered Indium8.9HF alloy and powder configuration is specified.

Key features

  • Stable Small-Aperture Transfer: High transfer efficiency through apertures at or below 0.66 area ratio supports fine-feature printing.
  • Clear Probe-Testable Residue: The no-clean residue supports in-circuit probe access after reflow.
  • Low-Voiding Reflow: The paste is formulated for low voiding in BGA, CSP, and QFN joints.

Applications / Suitable for

  • Fine-feature SMT stencil printing
  • BGA, CSP, and QFN assembly
  • Lead-free air or nitrogen reflow
Product Family

INDIUM 8.9HF

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Stencil Life
Up to 60 h hours

Additional Information

Technical properties

As-supplied / before-processing properties

Product-level handling and classification values for Indium8.9HF that do not depend on the unresolved alloy configuration.

Property Value Unit Method / condition
Flux classification ROL0 IPC J-STD-004B
Chlorine limit less than 900 ppm Halogen-free test per EN14582
Bromine limit less than 900 ppm Halogen-free test per EN14582
Total halogen limit less than 1,500 ppm IEC 61249-2-21; EN14582
Stencil life up to 12 hours 30 to 60% RH at 22 to 28 deg C
Shelf life 6 months Unopened container stored below 10 deg C