INDIUM 8.9E

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

INDIUM 8.9E

Main features

  • Fine-Aperture Print Transfer
  • Graping-Resistant Small Deposits
  • Low-Voiding BGA and CSP Reflow

Product Description

Indium8.9E Pb-Free Solder Paste is an air-reflow, no-clean solder paste for lead-free SMT assembly with SAC and other lead-free alloy systems. Its flux system combines high transfer efficiency through apertures at or below 0.66 area ratio with oxidation resistance that helps suppress incomplete coalescence on small deposits. The paste supports fine-feature printing, provides more than eight hours of stencil life under the stated temperature and humidity conditions, and is formulated for low voiding in BGA and CSP solder joints. Standard SAC305 and SAC387 offerings are available in multiple powder sizes. Applications include stencil printing and reflow for fine-pitch components, BGA packages, and CSP assemblies.

Key features

  • Fine-Aperture Transfer: High transfer efficiency through apertures at or below 0.66 area ratio supports small solder deposits.
  • Oxidation-Resistant Coalescence: Flux chemistry helps suppress graping on small deposits during lead-free reflow.
  • BGA and CSP Voiding Control: The paste is formulated for low voiding in BGA and CSP solder joints.

Applications / Suitable for

  • Fine-pitch SMT stencil printing
  • BGA and CSP assembly
  • Lead-free air or nitrogen reflow
Product Family

INDIUM 8.9E

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Stencil Life
More than 8 h hours

Additional Information

Technical properties

As-supplied / before-processing properties

Typical pre-reflow values for Indium8.9E; alloy and powder configuration are identified where they affect the value.

Property Value Unit Method / condition
Flux classification ROL1 J-STD-004A
Typical viscosity 1,450 poise Type 3 powder; Malcolm at 10 rpm
Typical viscosity 1,500 poise Type 4 powder; Malcolm at 10 rpm
Typical tackiness 35 g J-STD-005 test result
Stencil life greater than 8 hours 30 to 60% RH at 22 to 28 deg C
Shelf life 6 months Unopened container stored below 10 deg C