INDIUM 10.8HF

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

INDIUM 10.8HF

Main features

  • Broad Air-Reflow Process Window
  • Low-Voiding QFN and BGA
  • Halogen-Free ROL0 Flux System

Product Description

Indium10.8HF Pb-Free Solder Paste is a halogen-free, no-clean lead-free solder paste for surface-mount printing and air reflow. The ROL0 flux system supports broad lead-free process windows, high transfer efficiency, and controlled coalescence across Type 3, Type 4, Type 5, and T5-MC powder options. It is formulated for low voiding in QFN and BGA joints and leaves a clear residue after reflow. Under the stated shop conditions, stencil life extends up to 12 hours. Applications include lead-free SMT stencil printing and reflow where the ordered alloy, powder size, storage condition, and thermal profile are specified.

Key features

  • Broad Reflow Profile Window: The flux system supports lead-free air-reflow processing across documented profile conditions.
  • Low-Voiding QFN/BGA Reflow: The paste is formulated for low voiding in QFN and BGA solder joints.
  • Clear Post-Reflow Residue: The no-clean flux leaves a clear residue after the documented reflow process.

Applications / Suitable for

  • Lead-free SMT stencil printing
  • QFN and BGA assembly
  • Air reflow with the ordered alloy and powder configuration
Product Family

INDIUM 10.8HF

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

Other Properties
Stencil Life
Up to 12 h hours

Additional Information

Technical properties

As-supplied / before-processing properties

Typical pre-reflow values for Indium10.8HF; alloy, powder, package, storage, and environmental conditions are identified where they affect the value.

Property Value Unit Method / condition
Flux classification ROL0 IPC J-STD-004D
Typical viscosity 1,400 kcps Type 4 and Type 4.5 powder
Metal load 89 % Type 4 and Type 4.5 powder
Metal load 88.0 to 88.5 % Type 5 and T5-MC powder
Stencil life up to 12 hours 30 to 60% RH at 22 to 28 deg C
Shelf life 6 months Syringe stored below -10 deg C
Shelf life 6 months Jar or cartridge stored below 10 deg C
Halogen limits less than 900 Cl; less than 900 Br; less than 1,500 total ppm IEC 61249-2-21; EN14582