Hysol MG52F | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

MG52F Black Epoxy Mold Compound High Voltage Hysol MG52F | Black Epoxy Mold Compound Hysol MG52F Black Epoxy Mold Compound High Voltage

Main features

  • Designed for DL TSSOP packages
  • Designed for copper (Cu) leadframes
  • Excellent under biased humidity testing

Product Description

Hysol MG52F is a fast curing, high productivity molding compound, designed for high volume encapsulation of surface mount devices. MG52F is applicable for devices having chip dimensions up to 1 centimeter (400 mils) square. Various versions are available including MG52F-99B NXP which is designed to provide greatly improved moisture performance after preconditioning. It can be applied using both conventional and automold equipment.

Hysol MG52F was designed for and passed qualification testing on SOIC, PLCC, QFP, PDIP, 28, 48 and 56 pin TSSOP packages and has been used in production for more than 20 years. These packages had a copper leadframe with palladium plating. This material is designed to achieve JEDEC Level 1 requirements at 260°C reflow temperature on copper based, palladium-plated leadframes. Hysol MG52F meets UL 94 V-0 Flammability at 1/8 inch (3.18mm) thickness.

Hysol MG52F offers high adhesion to a wide range of substrates including Nickel and Palladium, low stress, a large operating window and molds with very low wire sweep. 

 

Product Family

HYSOL MG52F

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size and Pellet Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
78.8 %
Specific Gravity
1.84
Electrical Properties
Volume Resistivity
100000000000000000 Ohms⋅cm
Thermal Properties
Glass Transition Temperature (Tg)
155 °C
Thermal Conductivity
0.95 W/m.K
UL 94 Rating
V0
Mechanical Properties
Molded Shrinkage
0.3 %
Chemical Properties
Moisture absorption
0.57 %
Curing Conditions
Transfer Pressure
40 - 100 kg/cm2
Transfer Time
15 - 25 s
Physical Properties
Spiral Flow @ 175°C
76 cm

Additional Information

Hysol MG52F has excellent reliability and HTRB data and has successfully passed the following reliability tests:

  • Operating Life Static Test, 125° C, 5.5V 1000 Hours: Passed
  • Biased Humidity, 85° C / 85% R H, 1000 Hours: Passed
  • Autoclave, 121° C, 15 psi, 240 Hours: Passed
  • Temperature Cycle Test, -65° C to 150° C, 1000 Cycles: Passed
  • Storage Life Test, 150° C, 1000 Hours: Passed
  • Thermal Shock Test, -55° C to 125° C, 500 Cycles: Passed
  • Solder Heat, 260° C, 10 Sec, 1 Cycle: Passed
  • Lead Pull to Destruction: Passed
  • X-Ray: Passed

Leading Brands Trust in Our Products and Services