Hysol MG15F-0140B | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Hysol MG15F-0140B | Black Epoxy Mold Compound

Main features

  • Anhydride cured
  • Tg: 185°C
  • For power discretes and high voltage rectifiers

Product Description

Hysol MG15F-0140B is a black, semiconductor grade, anhydride curing epoxy molding compound designed for high voltage power applications requiring good electrical stability at high temperature. A real classic. The work horse, as the industry would call it, product of the halogen and anhydride containing chemistries.

Hysol MG15F-0140B was typically used for power discretes and high voltage rectifiers. Despite its glorious history, the industry has been leaning towards next generation compounds that are future proof while still maintaining the same, or sometimes even better mold properties. GR 750 and the GR 750 XX series in general have nothing to envy and are good drop in candidates for the old guard.

 

MG15F-0140B will be the successor of MG15F-0140 by the end of this year since it does not contain (Dechlorane Plus), which will be banned by the Chinese government by 2024.  
Product Family

HYSOL MG15F-0140B

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
black
Specific Gravity
1.81
Thermal Properties
Glass Transition Temperature (Tg)
185 °C
UL 94 Rating
V0
Physical Properties
Spiral Flow @ 175°C
56 cm
Curing Conditions
Transfer Pressure
42-84 kg/cm2
Transfer Time
6-15 s

Additional Information

Property Comparison Table of Hysol MG 15F-0140B vs Hysol MG15F-0140 

Property Unit MG 15F-0140B MG15F-0140
Gel time at 175°C s 18 17
Spiral flow at 175°C cm 56 56
Filler content % - 69
Shelf life at 5°C days 365 365
Preheat temperature (conventional mold) °C 77 to 94 75 to 95
Molding temperature °C 177 to 200 175 to 200
Molding pressure kgf/cm² 42 to 84 42 to 84
Transfer time s 6 to 15 6 to 15
Curing time (3 mm) at 177°C s 60 to 75 60 to 75
Curing time (3 mm) at 190°C s 45 to 60 45 to 60
Post cure time at 175°C h 8 to 12 8 to 12
Post cure time at 190°C h 2 to 4 2 to 6
Glass transition temperature (Tg) °C 185 195
CTE (alpha 1) below Tg ppm/°C 22 21
CTE (alpha 2) above Tg ppm/°C 57 70
Specific gravity - 1.81 1.81
Molded shrinkage % 0.34 0.2
Flexural strength MPa 115 127.5
Flexural modulus GPa 10.3 13.7
Thermal conductivity W/m-K - 0.65
Moisture absorption at 85°C/85% RH, 168 h % - 0.5
Volume resistivity at 500 V @ 21°C ohm-cm 4.3 × 1016 3.0 × 1016
Extractable ionic content: Chloride (Cl-) ppm 9.9 -
Extractable ionic content: Sodium (Na+) ppm 5 -
Water extract conductivity micromhos - 3
pH of extract - - 5.4
Flammability rating at 3 mm UL-94 V-0 V-0

Notes: Values are typical and should be confirmed against the latest product TDS and your process conditions. "-" indicates not yet available

This table summarizes and compares typical processing and cured-performance properties for two anhydride-cured epoxy molding compounds used in high-voltage power applications, showing that the molding window and cure conditions are broadly similar (gel time, spiral flow, transfer time, and cure schedules), while key material differences appear in thermo-mechanical and moisture-related behavior: MG15F-0140B reports lower Tg (195°C vs 185°C), lower CTE above Tg (70 vs 57 ppm/°C), lower flexural modulus (13.7 vs 10.3 GPa), but higher molded shrinkage (0.2% vs 0.34%), while both grades meet UL-94 V-0 at 3 mm and show high volume resistivity at 500 V and 21°C. 

 

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers