Hysol KL1000-3LX | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Hysol KL1000-3LX | Black Epoxy Mold Compound

Main features

  • High reliability
  • High moldability
  • Decreased cost-of-use

Product Description

Hysol KL1000-3LX is a black, semiconductor grade epoxy molding compound. It provides the lowest cost of ownership for an epoxy molding compound. It offers superior moldability and high reliability. This material is designed to satisfy JEDEC Level 4 requirements for reflow at 220 °C.

Hysol KL1000-3LX has a history that predates the acquisition of Huawei Electronics by Henkel. In 2005, Henkel formed a joint-venture with HuaweI Electronics in China to create Henkel Huawei Electronics (HHE) in Lianyungang China. HHE made low-end, halogen containing epoxy molding compounds that used Bromine or Antimony as a flame retardant. The KL1000-3LX is an old product that is still made at Hysol Huawei today. It meets UL94 V-0 flammability at a thickness of 3.175 mm. 

Hysol KL1000-3LX is a halogen-containing, legacy product that has been used for decades with great success for bridge rectifiers, axial packages, dual in line (DIP), TO packages, system in package (SiP), and SMX packages.

Product Family

HYSOL KL1000-3LX

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size and Pellet Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
75 %
Specific Gravity
2.02
Chemical Properties
Moisture absorption
0.23 %
Physical Properties
Spiral Flow @ 175°C
75 cm
Thermal Properties
Glass Transition Temperature (Tg)
165 °C
UL 94 Rating
V0
Electrical Properties
Volume Resistivity
1000000000000000 Ohms⋅cm
Curing Conditions
Transfer Pressure
40-100 kg/cm2
Transfer Time
10-18 s

Additional Information

Storage

Keep the product in its sealed container within a dry environment. Material that has been taken out of its containers can become contaminated while in use. Please refrain from putting the product back into the original container.

Powder or preforms must be stored in sealed containers at temperatures of 5 ºC or lower. When taking the material out of cold storage, it is crucial to allow it to reach room temperature inside the sealed container to prevent moisture contamination. For a standard 15 kg carton box, a recommended waiting time is 24 hours.