Hysol GR910-K | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Hysol GR910-K | Black Epoxy Mold Compound

Main features

  • Halogen free
  • High fluidity to avoid W/S issue
  • Designed for BGA/LGA

Product Description

Hysol GR910 K is a black epoxy molding compound specifically designed for Memory Ball Grid Arrays (BGA) and Land Grid Arrays (LGA). This semiconductor-grade material features spherical silica filler with a cut size of 53 µm, delivering exceptional fluidity and low shrinkage, which aids in advanced warpage control during manufacturing.

Hysol GR910 K is halogen-free and environmentally friendly, ensuring compliance with stringent safety standards. It offers excellent electrical performance, meeting the UL 94 V-0 flammability standard at a thickness of 1/8 inch.

Available Versions:

  • GR910 K | Optimized for high Tg and low modulus applications
  • GR910 K-31 | Tailored for high Tg and low shrinkage requirements

Key Features:

  • High Thermal Stability | Glass transition temperatures of 155°C (GR910 K) and 153°C (GR910 K-31)
  • Excellent Flowability | Ensures uniform coverage and filling during the molding process
  • Low Mold Shrinkage | 0.22% for GR910 K and 0.19% for GR910 K-31, contributing to precise dimensions
  • Low Coefficient of Thermal Expansion (CTE) | Minimizing stress during thermal cycling
  • Low Water Absorption | Less than 0.35%, enhancing reliability in humid environments

Highly Recommended For:

  • Advanced semiconductor packaging in high-performance applications
  • Memory devices requiring robust mechanical and thermal properties
  • Environmentally conscious projects where halogen-free materials are a must
Product Family

HYSOL GR910-K

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
86.5 %
Specific Gravity
1.97
Thermal Properties
Glass Transition Temperature (Tg)
155 °C
Thermal Conductivity
0.9 W/m.K
Electrical Properties
Volume Resistivity
40E15 Ohms⋅cm
Chemical Properties
Moisture absorption
0.35 %
Curing Conditions
Transfer Pressure
40 – 85 kg/cm2
Transfer Time
8 – 15 s
Physical Properties
Spiral Flow @ 175°C
200 cm

Additional Information

 
 GR910-K Series Product Properties Comparison
 
PROPERTY UNIT GR910 K GR910 K-31
Filler Content  % 86.5 89
Filler Cut um 53 53
Filler Shape - Spherical Spherical
Specific Gravity - 1.97 2.01
Spiral Flow  cm 200 172
Hot Plate Gel Time  sec 43 49
Glass Transition Temperature °C 155 153

CTE by TMA, α1

CTE by TMA, α2

ppm

ppm

10

37

9

32

Water Absorption (PCT24h)

wt%

0.35

0.33

Flexural Strength @25°C

Flexural Modulus @25°C

MPa

Gpa

141

19.8

145

24.5

Mold Shrinkage (After PMC)

%

0.22

0.19

Cl-

ppm 7 10
pH - 6.1 6.0
MSL Capability - MSL 2 MSL 3
Feature  

High Tg

Good Flowability

Low Modulus

High Tg

Low Shrinkage

Low CTE

 