Hysol GR910-C | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Hysol GR910-C | Black Epoxy Mold Compound

Main features

  • Halogen free
  • High fluidity
  • Designed for BGA/LGA

Product Description

Hysol GR910 C is a black, epoxy, semiconductor grade molding compound designed for Memory ball grid arrays (BGA) and land grid arrays (LGA). This spherical silica filled product (cut size of 75um), offers high fluidity and low shrinkage that aids a very advanced warpage control.

Hysol GR910 C is a halogen free, environmentally friendly compound with good electrical performance that meets UL 94 V-0 Flammability at 1/8 inch thickness. You might also be interested in GR910-C4 an identical product with even lower smile shrinkage.

Product Family

HYSOL GR910-C

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
88 %
Specific Gravity
2.01
Chemical Properties
Moisture absorption
0.3 %
Physical Properties
Spiral Flow @ 175°C
203 cm
Thermal Properties
Glass Transition Temperature (Tg)
130 °C
Thermal Conductivity
0.9 W/m.K
Curing Conditions
Transfer Pressure
40 - 85 kg/cm2
Transfer Time
7 - 15 s