Hysol GR825-73B | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

GR825-73B Black Epoxy Mold Compound for SOIC14 Hysol GR825-73B | Black Epoxy Mold Compound GR825-73B Black Epoxy Mold Compound for SOIC14 mini pellets

Main features

  • MSL 1 260°C
  • Designed for SOIC, SOP, SSOP & QSOP
  • Ideal for NiPdAu (PPF) & Ag-spot leadframes

Product Description

Hysol GR825-73B is approaching EOL and may be discontinued by 2023. The recommended alternative for SOIC packages is Hysol GR710F

Hysol GR825-73B is a black, semiconductor grade epoxy molding compound that was designed for SOIC packages. It was first qualified as MSL1 260°C on a 14 pin SOIC package with a die size of 1.4x 0.9mm (58 x 36 mils) using a Nickel Palladium Gold (NiPdAu) leadframe, also referred to as a preplated leadframe (PPF). It has since been used in mass production on this semiconductor package. Except for SOIC, it can also be used on, SOP, SSOP & QSOP packages.

Hysol GR825-73B is an environmentally friendly "green" molding compound which contains no bromine, antimony or phosphorus flame retardant and has been used in mass scale production since 2007. GR825-73B epoxy mold compound meets UL 94 V-0 Flammability at 3mm (1/8") thickness.

 
Product Family

HYSOL GR825-73B

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size and Pellet Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
80 %
Specific Gravity
1.9
Chemical Properties
Moisture absorption
0.32 %
Physical Properties
Spiral Flow @ 175°C
100 cm
Thermal Properties
Glass Transition Temperature (Tg)
135 °C
Thermal Conductivity
0.8 W/m.K
UL 94 Rating
V0
Electrical Properties
Dielectric Strength
37 kV/mm
Volume Resistivity
11000000000000000 Ohms⋅cm
Curing Conditions
Transfer Pressure
40 - 80 kg/cm2
Transfer Time
15 - 25 s