Hysol GR720 is a green, halogen-free epoxy molding compound specifically developed for SOT (Small Outline Transistor) packages with stringent requirements. GR720 sets new standards for performance and reliability in the electronics manufacturing realm. With a strong focus on die attach paste bonded SOT, GR720 excels in minimizing stress during bonding, ensuring the longevity of sensitive semiconductor components. Its low-stress formulation is a vital attribute, enhancing the durability of electronic devices.

Hysol GR720 its exceptional resistance to delamination, even after exposure to the rigorous conditions of MSL1 (Moisture Sensitivity Level 1) and TC1000 (Thermal Cycling at 1000 cycles). This outstanding performance guarantees the reliability of your devices, even when subjected to harsh environmental conditions. Moreover, Hysol GR720 offers exceptional workability, streamlining manufacturing operations and boosting overall efficiency.

Previously, packages molded with Hysol GR720 was able to achieve a Moisture Sensitivity Level (MSL) rating of 3 for die attach paste bonding. Additionally, it boasts remarkable filler properties with a filler content and cut of 84±1% and 75 µm, providing the best possible moldability and as wide a molding latitude as possible. HYSOL GR720 also meets UL94 V-0 Flammability at 1/8 inch thickness.

Product Family

HYSOL GR720

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
84 %
Specific Gravity
1.92
Thermal Properties
Glass Transition Temperature (Tg)
113 °C
Thermal Conductivity
0.92 W/m.K
UL 94 Rating
V-0
Electrical Properties
Volume Resistivity
26×10¹⁵ Ohms⋅cm
Chemical Properties
Moisture absorption
0.40 %
Physical Properties
Spiral Flow @ 175°C
119.38 cm
Curing Conditions
Transfer Pressure
40–85 kg/cm2
Transfer Time
7–15 s

Additional Information

Adhesion Strenght Data

Property Value Unit
Adhesion at RT to Cu Substrate after PMC  7.22 MPa
Adhesion at RT to Cu Substrate after Preconditioning 

6.82

MPa

 

Storage

Keep the product in its sealed container within a dry environment. Material that has been taken out of its containers can become contaminated while in use. Please refrain from putting the product back into the original container.

Optimal Storage: 5 °C. Storage greater than 5°C can adversely affect product properties.