Hysol GR700 C4C | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Hysol GR700 C4C | Black Epoxy Mold Compound

Main features

  • High reliability
  • High power applications
  • Good electrical performance

Product Description

Hysol GR700 C4C is a halogen free, black, silica filled (89% filler weight) semiconductor grade epoxy molding compound with a 75um filler cut size. This low stress, high adhesion compound has very good electrical performance and is currently under development, striving to provide high reliability for high power applications. This is a product that has achieved MSL 1 and its comparative tracking index (CTI) is 575V.

Hysol GR700 C4C is a green epoxy molding compound with excellent electrical performance, designed for high power devices applications with low moisture absorption requirements. Typical use can be found in SOP, DPAK, QFP, QFN semiconductor packages. Furthermore, it meets UL 94 V-0 flammability at 1/8 inch thickness.

Product Family

HYSOL GR700 C4C

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
89 %
Specific Gravity
2.00
Electrical Properties
Volume Resistivity
61000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.15 %
Physical Properties
Spiral Flow @ 175°C
114 cm
Thermal Properties
Glass Transition Temperature (Tg)
120 °C
Thermal Conductivity
0.9 W/m.K
UL 94 Rating
V0
Curing Conditions
Transfer Pressure
40 - 85 kg/cm2
Transfer Time
8 - 15 s

Additional Information