Hysol GR700 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Hysol GR700 | Black Epoxy Mold Compound

Main features

  • Low stress
  • For high power devices
  • Good electrical performance

Product Description

Hysol GR700, is a halogen free, black, silica filled (87% filler weight) semiconductor grade green epoxy molding compound designed for SOP MSL1. This low stress, high adhesion compound has very good electrical performance and is a proven, commercially available product code. This is a product that has achieved MSL 1 and its comparative tracking index (CTI) is 600V.

Hysol GR700 is a technologically advanced, halogen free, green epoxy molding compound with excellent electrical performance, designed for high power devices applications with low moisture absorption requirements. Typical use can be in SOP, DPAK,QFP, QFN, SOT semiconductor packages. Furthermore, it meets UL 94 V-0 flammability at 1/8 inch thickness..

HYSOL GR700 has been formulated to provide the best possible moldability and as wide a molding latitude as possible. Although molding and curing conditions will vary from situation to situation.


Available versions:

Product Family

HYSOL GR700

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.

Technical Specifications

General Properties
Color
Black
Filler Content
87 %
Specific Gravity
1.97
Thermal Properties
Glass Transition Temperature (Tg)
118 °C
Thermal Conductivity
0.9 W/m.K
UL 94 Rating
V-0
Electrical Properties
Volume Resistivity
60E15 Ohms⋅cm
Chemical Properties
Moisture absorption
0.26 %
Physical Properties
Spiral Flow @ 175°C
132.08 cm
Mechanical Properties
Molded Shrinkage
0.2 %
Curing Conditions
Transfer Pressure
40-85 kg/cm2
Transfer Time
8-15 s

Additional Information

GR700 Series for High-reliability Small Outline Packages

Leading Brands Trust in Our Products and Services