Hysol GR60 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Hysol GR60 | Black Epoxy Mold Compound

Main features

  • Designed for IPM application
  • Good moisture resistance
  • High thermal conductivity

Product Description

Hysol GR60 Series is a black semiconductor-grade epoxy molding compound designed for the encapsulation and protection of intelligent powder module (IPM) applications. With excellent workability and reliability, GR60 series is suitable for long wire or large body devices. With high thermal conductivity (1.7 ~ 2.2 W/mk), GR60 could be applied in SiC IGBT module with Tj 175°C and 1200V. More thermal conductive versions are also under development. Hysol GR60 is an environmentally "green" product, meaning that it doesn't contain any halogens including bromine, antimony or phosphorus flame retardants. Hysol GR60 meets UL 94 V-0 Flammability at 1/8 inch thickness. Key features are summarized as:

Reliability (check GR60 HT beta-site tests)

  • High adhesion to Cu/Ag/Ni
  • Low stress and low water absorption
  • High thermal conductivity 
  • Excellent performance in HAST, HTRB, TC, PCT, HTS, etc. 

Moldability

  • Excellent workability with wide process window
  • No wire sweep
  • Good warpage control

Available versions: GR60 HT, GR60 PT (check the GR60 comparison)

Suitable Package:  Full pack type IPM, substrate type IPM

Product Family

HYSOL GR60

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
black
Filler Content
87 %
Thermal Properties
Glass Transition Temperature (Tg)
107 °C
Thermal Conductivity
0.9 W/m.K
UL 94 Rating
V-0 @ 1/8 inch
Electrical Properties
Volume Resistivity
8300000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.34 %
Physical Properties
Spiral Flow @ 175°C
152.4 cm
Viscosity
13 mPa.s

Additional Information

Property GR60PT(98D69B) GR60PT(102A11) GR60HT GR60 (M1)
Filler content 83 86 86 87
Epoxy EOCN+LWA1 EOCN+LSR EOCN/LWA2 MAR+LWA2
Gel Time (sec) 32 30 40 30
Spiral Flow (inch) 40 29 24 60
Tg (°C) 172 117 119 107
CTE 1 20 15 19 8
CTE 2 61 49 44 29
Flexural Strength/Modulus, Mpa 116/ 17925 110/ 21112 137/ 19625 145/ 22580
DMA-Flexural Modulus (RT) 21141 25377 - 26971
DMA-Flexural Modulus (175/260°C) 2377/795 613/453 - 888/ 647
PCT 24hrs wt% 0.45 0.22 0.20 0.34
CI-, ppm 34 18 9 9
Na+, ppm 5 3 8 4
pH, ppm 7 7 6 5
Volume Resistivity, 10E15 Q 2 7 4.09 83
Thermal Conductivity, W/m.K 1.9 1.8 2.2 0.9

 

Epoxy Molding Compound For IPM Application

Hysol has developed different series (GR60 series, GR600 series, GR750 series, etc.) for IPM application. Highly conductive versions are also in development. 

Beside the common features, the two version GR60 PT and GR60 HT have their own unique features to meet niche requirements for your module. The differences between GR60 PT and GR60 HT:

  • Thermal conductivity: 1.7 W/mK (GR60 PT) v.s. 2.2 W/mK (GR60 HT)
  • Good adhesion to: Cu & Au surface (GR60 PT) v.s. Cu & Au & Ni surface (GR60 HT)
  • Others: high cost-efficient (GR60 PT) and good moisture resistance (GR60 HT)
 
  GR60 Series For IPM Application

Hysol GR60 series products are highly thermal conductive molding compounds designed for IPM applications. Both GR60 HT and GR60 PT are dedicated to module package with excellent workability and reliability, suitable for long wire or large body device.  The key common features of GR60HT and GR60PT are:

Workability

  • No wire sweep
  • Warpage control
  • Wide molding window

Great peformance

  • Good electrical stability during tests
  • High thermal conductivity
  • Flammability rating UL94 V-0 @1/8 inch
alt

GR60 HT Beta-Site Customer Evaluation 

alt

GR60 HT Release Force

alt

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers