Hysol GR30HT | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

GR30HT High Thermally Conductive Epoxy Molding Compound Duroplast Hysol GR30HT | Black Epoxy Mold Compound

Main features

  • High Thermal Conductivity GR30
  • Designed for TO92 and TO220 packages
  • Excellent reliability under high temperature and bias

Product Description

This product is no longer supplied. It has been replaced by GR350HT

Hysol GR30HT is a high thermal conductivity version of GR30. It is a black semiconductor-grade epoxy molding compound (duroplast) designed for the encapsulation and protection of TO92, TO3P, TO220 and TO247 power devices. Once molded and post-mold cured, this product provides optimum protection and reliability for these semiconductor devices. Compared to the standard GR30 version, which has a thermal conductivity of 0.95 W/mK, GR30HT boasts more than twice as much thermal conductivity with 1.95 W/mK while also maintaining the high performance and moldability enhancements over the GR300 roots.

Hysol GR30HT is an environmentally "green" product, meaning that it doesn't contain any bromine, antimony or phosphorus flame retardants. Previous MG-series EMC dominated the space for power semiconductors but used halogen-containing flame retardants. This next generation epoxy mold compound replaces these older generation products. This material is designed to achieve JEDEC Level 1 requirements at 260°C reflow temperature on Nickel or Nickel-plated leadframes. It also achieves UL 94 V-0 Flammability at 1/8 inch (3.18mm) thickness.

Product Family

HYSOL GR30HT

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
72 %
Specific Gravity
2.1
Physical Properties
Spiral Flow @ 175°C
88 cm
Thermal Properties
Glass Transition Temperature (Tg)
186 °C
Thermal Conductivity
1.9 W/m.K
UL 94 Rating
V0
Curing Conditions
Transfer Pressure
40 - 100 kg/cm2
Transfer Time
5 - 30 s

Additional Information

Designed for TO220 & TO247 devices

TO220 and TO247 are big, bulky packages, so molding these products with a standard mold compound is fairly easy without using any fine fillers. The trouble with these packages however is that epoxy mold compounds used typically fail High Temperature Reverse Bias (HTRB) testing, which exposes the device to humidity and temperature while the device is under BIAS. Devices often experience "gate leakage" under these conditions and fail catastrophically.

Furthermore, these devices are often used using a Nickel (Ni) leadframe, which is very difficult to adhere to. Therefore, epoxy moldng compound must have a very good adhesion to Nickel to achieve MSL1 preconditioning.


GR30HT Hysol High Thermal Conductivity EMC for Power Modules and TO Packages