Hysol GR300 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Hysol GR300 | Black Epoxy Mold Compound

Main features

  • Designed for TO220 & TO247 packages
  • Excellent HTRB performance
  • Excellent adhesion to Nickel (Ni) leadframes

Product Description

Hysol GR300 is a black semiconductor-grade epoxy molding compound designed for the encapsulation and protection of TO220 and TO247 power devices. Once molded and post-mold cured, this product provides optimum protection and reliability for these semiconductor devices. It exhibits good HTRB results and strikes an excellent balance of performance and moldability. While it is a great product, new developments have been made since its formulation so you might want also want to take a look at the new and improved Hysol GR30 that has better moldability and electrical properties.

Hysol GR300 is an environmentally "green" product, meaning that doesn't contain any bromine, antimony or phosphorus flame retardants. Previous MG-series EMC dominated the space for power semiconductors but used halogen-containing flame retardants. This next generation epoxy mold compound replaces these older generation products. This material is designed to achieve JEDEC Level 1 requirements at 260°C reflow temperature on Nickel or Nickel-plated leadframes. Hysol GR300 meets UL 94 V-0 Flammability at 1/8 inch (3.18mm) thickness.

Product Family

HYSOL GR300

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
80 %
Specific Gravity
1.94
Electrical Properties
Volume Resistivity
27000000000000000 Ohms⋅cm
Thermal Properties
Glass Transition Temperature (Tg)
185 °C
Thermal Conductivity
0.95 W/m.K
UL 94 Rating
V0
Chemical Properties
Moisture absorption
0.33 %
Curing Conditions
Transfer Pressure
40 - 100 kg/cm2
Transfer Time
5 - 30 s
Physical Properties
Spiral Flow @ 175°C
34 cm

Additional Information

Designed for TO220 & TO247 devices

TO220 and TO247 are big, bulky packages, so molding these products with a standard mold compound is fairly easy without using any fine fillers. The trouble with these packages however is that epoxy mold compounds used typically fail Hig Temperature Reverse Bias (HTRB) testing, which exposes the device to humidity and temperature while the device is under BIAS. Devices often experience "gate leakage" under these conditions and fail catastrophically.

Furthermore, these devices are often used using a Nickel (Ni) leadframe, which is very difficult to adhere to. Therefore, epoxy moldng compound must have a very good adhesion to Nickel to achieve MSL1 preconditoning.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers