Hysol GR2822 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Hysol GR2822 | Black Epoxy Mold Compound Hysol GR2822 | Black Epoxy Mold Compound

Main features

  • For Conductive Polymer Tantalum Solid Capacitors
  • Ultra-low stress epoxy mold compound
  • MSL3 260°C - Thin Wall Crack Resistance

Product Description

Hysol GR2822 is a silica filled (88%), black, epoxy molding compound. Despite what the name implies, it is not a newer version of 2820 but an improved version of our gold GR2811. Hysol GR2811 showed poor moisture resistance (crack after MSL3) and discolouration issues under harsh circumstances. GR 2822 was developed to solve those issues and while black, be used for demanding applications.

Hysol GR2822 heat curable EMC, meets JEDEC MSL 3 requirements and is a green product designed for tandalum conductive polymer capacitors. It exhibits very low stress, low moisture absorption and good electrical performance.

Product Family

HYSOL GR2822

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
88 %
Specific Gravity
1.98
Thermal Properties
Glass Transition Temperature (Tg)
105 °C
UL 94 Rating
V0
Electrical Properties
Volume Resistivity
14000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.26 %
Physical Properties
Spiral Flow @ 175°C
99 cm
Curing Conditions
Transfer Pressure
40 - 85 kg/cm2
Transfer Time
5 - 20 s

Additional Information

{tab=Applications}

Short Description of {product_name}

Typical applications and uses of {product_name} include:

  • Condutive Polymer Tantalum Solid Capacitors (POSCAP)
  • Other Tantalum Capacitors

Technical Datasheets for {product_name}

TDS (English) Kapton_Technical_Data_Sheet Click to access {product_name} Technical Data Sheet
*Note that only registered users may access technical datasheets

{tab=Packaging Details}

Packaging Details for {product_name}

The following information is specifically related to each unit of measure of {product_name}. If you which to compare this to other product sizes, click on the respective product from the list above and check here for values specific to that product. These values are taken from our internal database and are used in the calculation of the gross weight and packaging dimensions of the goods during shipping. You can use these values to approximate delivery charges using your own carrier.

{/tabs}

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers