Hysol GR2820 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

GR2820 Black Epoxy Mold Compound Hysol GR2820 | Black Epoxy Mold Compound

Main features

  • For Conductive Polymer Tantalum Solid Capacitors
  • Ultra-low stress
  • Thin Wall Crack Resistance

Product Description

Hysol GR2820 is a black, ultra low stress, semiconductor-grade epoxy molding compound designed for the encapsulation and protection of thin walled conductive polymer tantalum solid capacitors (POSCAP).  In the world of passive components, POSCAPs are relatively new to the scene. These solid electrolytic capacitors have many advantages, but offer challenges for epoxy mold compound manufacturers. After many years of development, the GR2820 has been developed to have excellent thin wall crack resistance - the greatest challenge of molding these devices. Furthermore, it has been optimized for automolding equipment.

Hysol GR2820 is a silica filled(81%) environmentally "green" halogen free product, meaning it doesn't contain any bromine, antimony or phosphorus flame retardants. Previous MG-series EMC dominated the space for tantalum capacitors but used halogen-containing flame retardants. This material is designed to achieve JEDEC Level 1 requirements at 260°C reflow temperature on conductive polymer capacitors. It's fast cure time also ensures that it is compatible with the latest automold manufacturing equipment. Hysol GR2820 meets UL 94 V-0 Flammability at 1/4 inch (6.35mm) thickness.

Product Family

HYSOL GR2820

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Filler Content
83 %
Specific Gravity
1.90
Electrical Properties
Volume Resistivity
16000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.37 %
Thermal Properties
Glass Transition Temperature (Tg)
183 °C
UL 94 Rating
V0
Curing Conditions
Transfer Pressure
40 - 100 kg/cm2
Transfer Time
6 - 18 s
Physical Properties
Spiral Flow @ 175°C
66 cm

Additional Information

{tab=Applications}

Short Description of {product_name}

Typical applications and uses of {product_name} include:

  • Condutive Polymer Tantalum Solid Capacitors (POSCAP)
  • Other Tantalum Capacitors

Technical Datasheets for {product_name}

TDS (English) Kapton_Technical_Data_Sheet Click to access {product_name} Technical Data Sheet
*Note that only registered users may access technical datasheets

{tab=Packaging Details}

Packaging Details for {product_name}

The following information is specifically related to each unit of measure of {product_name}. If you which to compare this to other product sizes, click on the respective product from the list above and check here for values specific to that product. These values are taken from our internal database and are used in the calculation of the gross weight and packaging dimensions of the goods during shipping. You can use these values to approximate delivery charges using your own carrier.