Hysol GR2811 | Gold Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

GR2811 Gold Epoxy Mold Compound Hysol GR2811 | Gold Epoxy Mold Compound

Main features

  • Very low stress
  • Gold (yellow) colored
  • Thin Wall Crack Resistance

Product Description

Hysol GR 2811 is a yellow - gold semiconductor epoxy molding compound designed for the encapsulation and protection of thin walled conductive polymer tantalum solid capacitors (POSCAP). Once molded and post-mold cured, this product provides optimum protection and reliability for these capacitor devices

Hysol GR 2811 is Designed for Conductive Polymer Tantalum Solid Capacitors (POSCAP). In the world of passive components, POSCAPs are relatively new to the scene. These solid electrolytic capacitors have many advantages, but offer challenges for epoxy mold compound manufacturers. After many years of development, the GR 2811 has been developed to have excellent thin wall crack resistance - the greatest challenge of molding these devices. Furthermore, it has been optimized for automolding equipment.

Hysol GR 2811 is an environmentally "green" product, meaning that it doesn't contain any bromine, antimony or phosphorus flame retardants. MG33F-0520 and MG33F-0602 dominated the space for tantalum capacitors but used halogen-containing flame retardants. This next generation epoxy mold compound replaces these older generation products.This material is designed to achieve JEDEC Level 1 requirements at 260°C reflow temperature on conductive polymer capacitors. It's fast cure time also ensures that it is compatible with the latest automold manufacturing equipment. Hysol GR 2811 meets UL 94 V-0 Flammability at 1/4 inch (6.35mm) thickness.

 

 

Product Family

HYSOL GR2811

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Gold
Filler Content
85 %
Specific Gravity
1.96
Electrical Properties
Volume Resistivity
10000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.35 %
Physical Properties
Spiral Flow @ 175°C
86.36 cm
Thermal Properties
Glass Transition Temperature (Tg)
162 °C
Thermal Conductivity
2.7 W/m.K
UL 94 Rating
V0
Mechanical Properties
Molded Shrinkage
0.1 %
Curing Conditions
Transfer Pressure
40 - 85 kg/cm2
Transfer Time
5 - 15 s

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers