HumiSeal 1R32A-2/505 Acrylic Conformal Coating is a fast-drying, single-component acrylic conformal coating pre-blend for printed circuit assemblies. The ready-to-use liquid supports automated coating processes and can also be applied by dipping, spraying, or brushing after the ordered PB viscosity grade is confirmed. It dries to handling condition in 10 minutes under the stated test method and develops a clear protective film with ultraviolet fluorescence for inspection. The coating is used where acrylic moisture and environmental protection are required on circuit boards, components, and electronic assemblies while retaining practical repair access.

Key features

  • Fast-Drying Acrylic Film: The coating reaches handling condition in 10 minutes under ASTM D1640.
  • Ready-to-Use Pre-Blend: The /505 format supports direct coating after confirming the ordered PB viscosity grade.
  • UV Inspection Fluorescence: Ultraviolet fluorescence supports visual verification of coating coverage.

Applications / Suitable for

  • Printed circuit assembly conformal coating
  • Automated film coating after PB grade confirmation
  • Dipping, spraying, or brushing of electronic assemblies
Product Family

HUMISEAL 1R32A-2/505

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.91 g/cm3
Solids
29 %
Thermal Properties
Glass Transition Temperature (Tg)
14 °C
Operating Temperature
-65 - 125 °C
Electrical Properties
Breakdown Voltage
7500 V

Additional Information

Technical properties

As-supplied / before-processing properties

Typical product-level handling values for the 1R32A-2/505 pre-blend family; grade-specific liquid properties are omitted because the ordered PB viscosity grade is not identified.

Property Value Unit Method / condition
Shelf life 12 months Pre-blend shelf life
Storage temperature 0 to 35 deg C Tightly closed container
Pre-use equilibration 24 hours 18 to 32 deg C before use
Drying time to handle 10 minutes ASTM D1640
Technical properties

After-processing / final-state properties

Typical processed-coating values for HumiSeal 1R32A-2/505; cure conditions and test methods are retained where they affect interpretation.

Property Value Unit Method / condition
Recommended coating thickness 25 to 75 um Applied coating thickness
Recommended cure 24 hours Room temperature
Accelerated cure 2 hours 76 deg C
Time to optimum properties 7 days After application
Thermal shock range -65 to 125 deg C 50 cycles; MIL-I-46058C
Glass transition temperature 14 deg C DSC
Flammability V-0 UL 94
Dielectric withstand voltage greater than 1,500 V MIL-I-46058C