HUMISEAL 1B51NSLU/521EU

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

HUMISEAL 1B51NSLU/521EU

Main features

  • 521EU Thinner Compatibility
  • Low-Permeability Flexible Film
  • Room-Temperature and Heat Cure

Product Description

HumiSeal 1B51NSLU/521EU Synthetic Rubber Conformal Coating is a fast-drying single-component synthetic rubber conformal coating used with HumiSeal 521EU thinner for printed circuit assembly protection. The 1B51NSLU coating uses a methylcyclohexane solvent system and forms a flexible, UV-fluorescent, repairable film with low moisture-vapor permeability. Compatible thinner options include 903, 905, and 521EU. The recommended coating thickness is 25 to 75 um, with cure completed in 24 hours at room temperature or 30 minutes at 76 deg C. The cured coating is stated for thermal-shock exposure from -65 to 125 deg C.

Key features

  • 521EU application-thinner compatibility: The coating is supported with HumiSeal 521EU for application-viscosity adjustment.
  • Flexible UV-inspectable film: The final synthetic rubber film is flexible, UV fluorescent, and repairable.
  • Room-temperature or accelerated cure: The coating cures in 24 hours at room temperature or 30 minutes at 76 deg C.

Applications

  • Conformal coating of printed circuit assemblies
  • Moisture and environmental protection of electronic assemblies
Product Family

HUMISEAL 1B51NSLU/521EU

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.81 g/cm3
Solids
15 %
Thermal Properties
Glass Transition Temperature (Tg)
14 °C
Operating Temperature
-65 - 125 °C
Electrical Properties
Breakdown Voltage
4900 V

Additional Information

Technical properties

As-supplied / before-processing properties

Supported base-coating composition, thinner compatibility, and shelf-life data before application.

Property Value Unit Method / condition
Product form Single-component liquid coating - 1B51NSLU base coating
Base polymer Synthetic rubber - As supplied
Solvent system Methylcyclohexane - As supplied
Compatible thinners 903; 905; 521EU - Application-viscosity adjustment
Shelf life at room temperature 18 months 1B51NSLU base coating
Inspection aid UV fluorescence - Optical brightener in the coating
Technical properties

After-processing / final-state properties

Supported applied-film and cured-coating characteristics for the 1B51NSLU system.

Property Value Unit Method / condition
Recommended coating thickness 25 to 75 um Applied conformal coating
Recommended cure 24 h at room temperature or 30 min at 76 deg C - Cure schedule
Thermal-shock range -65 to 125 deg C stated cured-coating exposure
Glass transition temperature 14 deg C Typical cured coating
Moisture-vapor behavior Low permeability - Cured synthetic rubber film
Flexibility Flexible - Cured film
Inspection aid UV fluorescence - Cured film
Repairability Repairable - Cured film