HUMISEAL 1B51NS-60

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

HUMISEAL 1B51NS-60

Main features

  • Low Moisture-Vapor Transmission
  • Rapid Synthetic-Rubber Handling
  • Flexible Low-Stress Protection

Product Description

HumiSeal 1B51NS-60 Synthetic Rubber Conformal Coating is a fast-drying single-component synthetic rubber conformal coating for printed circuit assemblies. The liquid has a density of 0.81 +/- 0.02 g/cm^3, 22 +/- 1.5% solids, and a viscosity of 185 +/- 30 cP. It dries to handle in 10 minutes and is applied at a recommended thickness of 25 to 75 um. The cured film is flexible, low stress, repairable, and has very low moisture-vapor permeability. Cure is completed in 24 hours at room temperature or 30 minutes at 76 deg C.

Key features

  • Low moisture-vapor permeability: The synthetic rubber film has documented moisture-vapor transmission below 1 g/(m^2 day mil).
  • Ten-minute dry-to-handle time: The coating reaches the documented handling stage in 10 minutes.
  • Flexible low-stress film: The cured coating is flexible, low stress, and repairable.

Applications

  • Conformal coating of printed circuit assemblies
  • Moisture and environmental protection of electronic assemblies
Product Family

HUMISEAL 1B51NS-60

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.81 g/cm3
Solids
22 %
Thickness range
0.025-0.075 mm
Physical Properties
Viscosity
850 mPa.s
VOC
632 grams/liters
Electrical Properties
Breakdown Voltage
4900 V
Thermal Properties
Glass Transition Temperature (Tg)
14 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid, handling, and shelf-life data before application.

Property Value Unit Method / condition
Density 0.81 +/- 0.02 g/cm^3 ASTM D1475
Solids content 22 +/- 1.5 % by weight Fed-Std-141 method 4044
Viscosity 185 +/- 30 cP Fed-Std-141 method 4287
VOC 632 g/L As supplied
Drying time to handle 10 min Fed-Std-141 method 4061
Shelf life at room temperature 18 months From date of manufacture
Technical properties

After-processing / final-state properties

Typical cured-film, environmental, and electrical properties after the stated cure.

Property Value Unit Method / condition
Recommended coating thickness 25 to 75 um Applied conformal coating
Recommended cure 24 h at room temperature or 30 min at 76 deg C - Cure schedule
Time to optimum properties 7 days After application
Thermal shock -65 to 125 deg C 50 cycles per MIL-I-46058C
Glass transition temperature 14 deg C DSC
Coefficient of thermal expansion 55 ppm/deg C TMA
Moisture-vapor transmission < 1 g/(m^2 day mil) ASTM E398-03
Dielectric withstand voltage > 1500 V MIL-I-46058C
Dielectric breakdown voltage 4900 V ASTM D149
Insulation resistance 2.0 x 10^14 ohm MIL-I-46058C
Fungus resistance Passes - ASTM G21