HumiSeal 1B31S Acrylic Conformal Coating

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

HumiSeal 1B31S Acrylic Conformal Coating

Main features

  • MIL‑I‑46058C qualified
  • IPC‑CC‑830 compliant
  • RoHS compliant (Directive 2002/95/EC)

Product Description

HumiSeal 1B31S is a fast‑drying, single‑component acrylic conformal coating with improved adhesion and excellent moisture and environmental protection for printed circuit assemblies. The coating offers outstanding flexibility, fluoresces under UV light for streamlined inspection, and is easily repairable. HumiSeal 1B31S is MIL‑I‑46058C qualified, IPC‑CC‑830 compliant, and RoHS Directive 2002/95/EC compliant.

Product Key Features

  • Single‑component acrylic formulation
  • Fast drying for efficient throughput
  • MIL‑I‑46058C qualified
  • IPC‑CC‑830 compliant
  • RoHS compliant (Directive 2002/95/EC)

Applications

Product Family

HUMISEAL 1B31S

1. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 6 weeks
Packaging
Please select Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.91 g/cm3
Film Thickness
25 - 75 µm
Solids
35 %
Physical Properties
Viscosity
200 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
14 °C
Operating Temperature
-65 - 125 °C
UL 94 Rating
HB
Electrical Properties
Breakdown Voltage
7500 V