HUMISEAL 1B31-S

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

HUMISEAL 1B31-S

Main features

  • Rapid Acrylic Film Handling
  • UV-Assisted Coating Inspection
  • Ambient or Accelerated Cure

Product Description

HumiSeal 1B31S Acrylic Conformal Coating is a fast-drying single-component acrylic conformal coating for moisture and environmental protection of printed circuit assemblies. The liquid has a density of 0.91 +/- 0.02 g/cm^3, 35 +/- 3% solids, and a viscosity of 200 +/- 15 cP. It dries to handle in 10 minutes and is applied at a recommended thickness of 25 to 75 um. The coating cures in 24 hours at room temperature or 30 minutes at 76 deg C, fluoresces under UV for inspection, remains flexible, and can be repaired.

Key features

  • Ten-minute dry-to-handle time: The coating reaches the documented handling stage in 10 minutes.
  • Flexible UV-inspectable film: The cured acrylic film is flexible and fluoresces under UV for inspection.
  • Room-temperature or accelerated cure: The coating cures in 24 hours at room temperature or 30 minutes at 76 deg C.

Applications

  • Conformal coating of printed circuit assemblies
  • Moisture and environmental protection of electronic assemblies
Product Family

HUMISEAL 1B31-S

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.91 g/cm3
Solids
35 %
Thickness range
0.025-0.075 mm
Physical Properties
Viscosity
200 mPa.s
VOC
592 grams/liters
Electrical Properties
Breakdown Voltage
7500 V
Thermal Properties
Glass Transition Temperature (Tg)
14 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid, handling, and shelf-life data before application.

Property Value Unit Method / condition
Density 0.91 +/- 0.02 g/cm^3 Typical liquid value
Solids content 35 +/- 3 % by weight As supplied
Viscosity 200 +/- 15 cP Typical liquid value
VOC 592 g/L As supplied
Drying time to handle 10 min Fed-Std-141 method 4061
Shelf life at room temperature 24 months From date of manufacture
Technical properties

After-processing / final-state properties

Typical applied-film and cured-coating properties after the stated cure.

Property Value Unit Method / condition
Recommended coating thickness 25 to 75 um Applied conformal coating
Recommended cure 24 h at room temperature or 30 min at 76 deg C - Cure schedule
Time to optimum properties 7 days After application
Thermal-shock range -65 to 125 deg C Thermal-shock exposure
Glass transition temperature 14 deg C Typical cured coating
Inspection aid UV fluorescence - Cured film
Flexibility Flexible - Cured film
Repairability Repairable - Cured film