HumiSeal 1A33NS Urethane Conformal Coating

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

HumiSeal 1A33NS Urethane Conformal Coating

Main features

  • Fluoresces under UV light for inspection
  • Low moisture vapor permeability
  • Fast drying to handle (15 minutes)

Product Description

HumiSeal 1A33NS is a high-performance, toluene-free polyurethane coating designed for the most demanding electronic environments. Offering a safer, isocyanate-free alternative for the workshop, it provides a robust shield against moisture and chemical contaminants. Whether for automotive sensors or military hardware, 1A33NS ensures reliable performance with the added benefit of UV traceability and UL-certified protection.

Product Key Features

  • Single-component polyurethane conformal coating
  • Toluene-free formulation
  • No free isocyanates
  • Fluoresces under UV light for inspection
  • Fast drying to handle (15 minutes)
  • Low moisture vapor permeability
  • RoHS Directive 2002/95/EC compliant

Applications

Product Family

HUMISEAL 1A33NS

1. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 6 weeks
Packaging
Please select Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.95 g/cm3
Film Thickness
25 - 75 µm
Solids
44 %
Physical Properties
Viscosity
180 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
26 °C
Operating Temperature
-65 - 125 °C
Electrical Properties
Breakdown Voltage
7500 V

Additional Information

Learn More About HumiSeal® 1A33NS

Application Methods

HumiSeal® 1A33NS can be applied using standard conformal coating techniques. Proper substrate cleanliness is essential to ensure coating performance and reliability.

  • Dipping: Viscosity may be adjusted using HumiSeal® Thinner 521 to achieve a uniform film. Use a controlled immersion and withdrawal rate of 5–15 cm/min. Monitor viscosity regularly using a Zahn or Ford cup.

  • Spraying: Apply using conventional spray equipment with adequate ventilation. A typical starting ratio is 1:1 by volume of coating to Thinner 521, adjusted as needed to achieve a pinhole-free film.

  • Brushing: Suitable for localized coating or repair. Film uniformity depends on component density and operator technique.

Important Notes:

  • Surfaces must be free of moisture, grease, flux residues, and contaminants
  • Viscosity should be checked regularly during application
  • Perform process validation prior to full production use

Application Compatibility

HumiSeal® 1A33NS is compatible with materials commonly used in electronic assemblies.

Compatible With:
✔ FR-4 and standard PCB substrates
✔ Copper, tin, nickel, and plated finishes
✔ Most electronic components
✔ Automated and manual coating equipment

Not Recommended For:
✖ Contaminated or moisture-laden substrates
✖ Use near open flames or ignition sources

Additional Guidance:
UV fluorescence enables easy inspection and verification of coating coverage. Always confirm compatibility with assembly materials and processes.


Safety and Handling Precautions ⚠️

  • Use only in well-ventilated areas
  • Avoid inhalation of vapors or spray mist
  • Avoid contact with skin and eyes
  • Keep away from sparks, heat, and open flames
  • Follow all local and national safety regulations

Always consult the Safety Data Sheet (SDS) before use.

Storage Recommendations 📦

Store HumiSeal® 1A33NS in tightly closed containers away from excessive heat or cold. Recommended storage temperature is 0–35°C. Allow the product to equilibrate for 24 hours at 18–32°C prior to use.


Compliance You Can Trust ✅

HumiSeal® 1A33NS meets key industry and regulatory requirements:

✔ RoHS Directive 2002/95/EC compliant
✔ Toluene-free formulation
✔ No free isocyanates
✔ UV fluorescent for inspection and quality control