HumiSeal 1A33LOS Urethane Conformal Coating

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

HumiSeal 1A33LOS Urethane Conformal Coating

Main features

  • Fluoresces under UV light for easy inspection
  • Low moisture vapor permeability
  • No free isocyanates

Product Description

HumiSeal 1A33LOS is a high-performance, single-component polyurethane coating that eliminates the safety risks associated with traditional isocyanates. Ideal for high-reliability PCBs, it provides a tough, chemical-resistant shield while remaining low-odor and low-toxicity. With UV fluorescence for inspection and full RoHS compliance, it offers a "no-compromise" transition from standard 1A33 to a safer, more sustainable production process.

Product Key Features

  • Single-component polyurethane conformal coating
  • Reduced odor formulation with lower toxicity solvents
  • Comparable cured performance to HumiSeal 1A33
  • Fluoresces under UV light for easy inspection
  • No free isocyanates
  • Low moisture vapor permeability
  • Available in ready-to-use pre-blended viscosities
  • RoHS Directive 2015/863/EU and China RoHS 2 compliant

Applications

  • Printed circuit board (PCB) protection
  • Consumer electronics assemblies
  • Industrial electronics
  • Telecommunications equipment
  • Automotive electronic modules
  • Power supply assemblies
  • Electronic assemblies requiring low-odor coatings
Product Family

HUMISEAL 1A33LOS

1. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 6 weeks
Packaging
Please select Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.92 g/cm3
Film Thickness
25 - 75 µm
Solids
44 %
Physical Properties
Viscosity
195 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
26 °C
Operating Temperature
-65 - 125 °C

Additional Information

Learn More About HumiSeal® 1A33LOS

Application Methods

HumiSeal® 1A33LOS is available in pre-blended viscosities for immediate use, supporting multiple application techniques.

  • Dipping: Apply using a controlled immersion and withdrawal rate of 5–15 cm/min to ensure uniform coating thickness. Monitor viscosity regularly and adjust with approved thinner as needed.

  • Spraying: Pre-blended grades can be sprayed using conventional spray equipment. Adequate ventilation is required to remove solvent vapors and mist.

  • Brushing: Suitable pre-blends may be applied by brush. Film uniformity depends on viscosity selection and operator technique.

Important Notes:

  • Substrate cleanliness is critical for coating performance.
  • Perform compatibility testing prior to production use.
  • Consult HumiSeal® Technical Support for pre-blend selection.

Application Compatibility

HumiSeal® 1A33LOS is compatible with a wide range of materials used in electronic assemblies.

Compatible With:
✔ FR-4 and common PCB substrates
✔ Metals and plated finishes
✔ Most electronic components
✔ Automated coating equipment

Not Recommended For:
✖ Contaminated or moisture-laden substrates
✖ Application near open flames or ignition sources

Additional Guidance:
Always verify material compatibility and cleanliness prior to coating. UV fluorescence allows easy inspection and repair after application.


Safety and Handling Precautions ⚠️

  • Use only in well-ventilated areas
  • Avoid inhalation of vapors or spray mist
  • Avoid contact with skin and eyes
  • Keep away from sparks, heat, and open flames
  • Follow local and national health and safety regulations

Always consult the Safety Data Sheet (SDS) before use.

Storage Recommendations 📦

Store HumiSeal® 1A33LOS and its pre-blends in tightly closed containers away from excessive heat or cold. Recommended storage temperature is 0–35°C. Allow material to equilibrate for 24 hours at 18–32°C before use.


Compliance You Can Trust ✅

HumiSeal® 1A33LOS meets international reliability and compliance standards:

✔ RoHS Directive 2015/863/EU compliant
✔ China RoHS 2 compliant
✔ No free isocyanates
✔ UV fluorescent for inspection and quality control

Leading Brands Trust in Our Products and Services