HUMISEAL 1A33/521PB65 URETHANE CONFORMAL COATING

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

HUMISEAL 1A33/521PB65 URETHANE CONFORMAL COATING

Main features

  • 67.5 +/- 2.5 cP Preblend
  • Printed-Circuit-Assembly Moisture Protection
  • IPC, MIL, and UL Compliance

Product Description

HumiSeal® 1A33/521 PB 65 CPS Urethane Conformal Coating is a single-component polyurethane conformal coating pre-blended to a viscosity suitable for immediate application without additional dilution. Designed for general printed circuit board applications, it provides protection against moisture, salt, corrosive environments, and dirt while maintaining low moisture-vapor permeability. Once fully cured, the pre-blend provides properties equivalent to HumiSeal® 1A33 and supports UV inspection and localized repair. The coating meets MIL-I-46058C, IPC-CC-830B, IEC 60664-3, UL 746E, and UL 94 V-0 requirements and is recognized under UL file E105698.

Key features

  • Pre-blended application viscosity: Supplied at 67.5 ± 2.5 cPs for immediate use without additional dilution.
  • Environmental protection: Provides protection against moisture, salt, corrosive environments, and dirt with low moisture-vapor permeability.
  • Inspection and repair support: Fluoresces under UV light to assist coating inspection and is designed to be repairable.

Applications / Suitable for

  • General printed circuit board conformal coating applications
  • Protection of electronic assemblies from moisture, salt, corrosive environments, and dirt
  • Applications requiring UV-assisted coating inspection
Product Family

HUMISEAL 1A33/521PB65

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Thickness range
0.025-0.075 mm
Thermal Properties
UL 94 Rating
V-0
Electrical Properties
Breakdown Voltage
7,500 V

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid-coating and handling properties for HumiSeal® 1A33/521 PB 65 CPS. Values are not intended for use as specifications.

Property Value Unit Method / condition
Product form Single-component polyurethane conformal coating pre-blend — As supplied; no additional dilution required
Viscosity 67.5 ± 2.5 cPs Liquid coating
Solids content 40 ± 2 % Liquid coating
Density 0.93 ± 0.02 g/cm³ Liquid coating
VOC 558.0 g/L Liquid coating
Drying time to handle 15 minutes Fed-Std-141, Method 4061
Shelf life 24 months From date of manufacture; store tightly closed at 0 to 35°C
Technical properties

After-processing / final-state properties

Typical fully cured properties shared by HumiSeal® 1A33 and its pre-blends. Values are not intended for use as specifications.

Property Value Unit Method / condition
Recommended coating thickness 25–75 microns Cured coating
Optional curing conditions to reach optimum properties 30 days; 30 hours; or 20 hours — 30 days at room temperature; 30 hours at 76°C; or 20 hours at 88°C
Thermal shock 50 cycles — MIL-I-46058C; −65°C to 125°C
Glass transition temperature 26 °C DSC
Flammability V-0 — UL 94
Dielectric breakdown voltage 7500 volts ASTM D149
Dielectric constant 3.6 — ASTM D150-98; 1 MHz and 25°C
Moisture insulation resistance 1.6 × 1010 (16 GΩ) ohms MIL-I-46058C

Leading Brands Trust in Our Products and Services