HARDENER HY 8683

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

HARDENER HY 8683

Main features

  • Fast-Setting Polyurea for Filter Bonding
  • 15-Minute Working Window
  • 475% Elongation with 100 Pli Peel

Product Description

ARALDITE® AY 8683 Resin / Hardener HY 8683 is a two-component polyurea elastomeric adhesive formulated for filter-bonding applications. The fast-setting system cures at room temperature and can be mixed by hand or processed through meter-mix equipment. A 100:60 resin-to-hardener ratio by weight or volume, 15-minute pot life at 77°F (25°C) for a 90 g mass, and typical mixed viscosity of 2,500–3,000 cP support dispensing and assembly. After a seven-day room-temperature cure, typical properties include Shore A 95 ± 5 hardness, 475% ultimate elongation, and 100 pli floating roller peel. The cured adhesive is tough and resilient.

Key features

  • Filter-bonding formulation: Two-component polyurea elastomeric adhesive developed for filter assembly applications.
  • Controlled two-component processing: Uses a 100:60 resin-to-hardener ratio by weight or volume with a typical 15-minute pot life at 77°F (25°C).
  • Resilient cured performance: Typical cured properties include 475% elongation and 100 pli floating roller peel under the stated test conditions.

Applications / Suitable for

  • Filter bonding
Product Family

HARDENER HY 8683

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Blue
Specific Gravity
1.03
Physical Properties
Viscosity
75 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values tested at 77°F (25°C) unless otherwise stated. Resin, hardener, and mixed-material properties are identified separately.

Property Value Unit Method / condition
Color / appearance Milky white / blue liquid — AY 8683 Resin / HY 8683 Hardener; visual
Specific gravity 1.03 / 1.03 — AY 8683 Resin / HY 8683 Hardener; ASTM D-792
Resin viscosity 8,000–12,000 cP AY 8683 Resin at 77°F (25°C); ASTM D-2393
Hardener viscosity 60–90 cP HY 8683 Hardener at 77°F (25°C); ASTM D-2393
Resin-to-hardener mix ratio 100:60 Parts By weight and by volume
Pot life 15 min Mixed 90 g mass at 77°F (25°C); ASTM D-2471
Mixed viscosity 2,500–3,000 cP At 77°F (25°C); ASTM D-2393
Minimum cure time 24 h Recommended cure at 77°F (25°C)
Technical properties

After-processing / final-state properties

Typical values are not for specification purposes. Specimens were cured for seven days at 77°F (25°C) and tested at 77°F (25°C) unless otherwise stated.

Property Value Unit Method / condition
Hardness 95 ± 5 Shore A ASTM D-2240
Tensile strength 3,500 (24.1) psi (MPa) ASTM D-638; test rate 20 in./min (50 cm/min)
Ultimate elongation 475 % ASTM D-638; test rate 20 in./min (50 cm/min)
Tear strength 375 (65.6) ppi (N/mm) ASTM D-624; test rate 20 in./min (50 cm/min)
Floating roller peel 100 (17.5) pli (N/mm) ASTM D3167-03a