HARDENER HW 8680

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

HARDENER HW 8680

Main features

  • 225% Cured Elongation
  • Polycarbonate, Nylon, and Primed-Metal Bonding
  • 1:1 Mix with 15-Minute Open Time

Product Description

Araldite® AW 8680 Resin / Hardener HW 8680 is a general-purpose, two-part polyurethane adhesive designed for bonding a wide variety of substrates. It provides a long open time and cures to form a highly flexible bond, making it particularly well suited for primed metals and plastics such as polycarbonate and nylon.

Key features

  • Excellent flexibility: Delivers highly flexible bonds with an elongation of 225% once fully cured.
  • Convenient processing: Features an easy-to-use 1:1 mix ratio by volume for straightforward application.
  • Extended open time: Offers a 15-minute pot life at 77°F (25°C), providing ample time for assembly.

Applications / Suitable for

  • General plastic bonding.
  • Bonding polycarbonate and nylon headlamps.
  • Primed metal bonding applications.
Product Family

HARDENER HW 8680

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Mix Ratio
1:1
Pot Life
30 minutes
Mechanical Properties
Elongation
15 %

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure processing characteristics of mixed Araldite® AW 8680 / HW 8680.

Property Value Unit Method / condition
Mix Ratio (Volume) 1:1 (100:100) - Resin to Hardener
Mix Ratio (Weight) 93:100 - Resin to Hardener
Viscosity (Mixed) 50,000 cP at 77°F (25°C), ASTM D-2393
Pot Life 15 minutes at 77°F (25°C), 100 gram mass, ASTM D-2471
Sag Resistance 3/8 (10) inches (mm) 30° angle, 230°F (110°C), 30 min
Technical properties

After-processing / final-state properties

Cured mechanical and thermal properties of Araldite® AW 8680 / HW 8680.

Property Value Unit Method / condition
Hardness 30 Shore D ASTM D-2240, tested at 77°F (25°C)
Ultimate Tensile Strength 1100 (7.6) psi (MPa) ASTM D-638, tested at 77°F (25°C)
Elongation 225 % ASTM D-638, tested at 77°F (25°C)
Glass Transition Temperature (Tg) 104 (40) °F (°C) DMA, ASTM D-4065, tested at 77°F (25°C)
Lap Shear Strength (Nylon) 350 (2.4) psi (MPa) ASTM D1002, Cured 20 min @ 212°F (100°C), tested at 77°F (25°C)
Lap Shear Strength (Polycarbonate) 300 (2) psi (MPa) ASTM D1002, Cured 20 min @ 212°F (100°C), tested at 77°F (25°C)