HARDENER HV 8503

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

HARDENER HV 8503

Main features

  • One-Minute Fixturing Time
  • Heat-Resistant Curing Service
  • 1:1 Controlled Mixing

Product Description

Araldite® AV 8503 Resin / Hardener HV 8503 is a two-component epoxy adhesive paste designed primarily for bonding sheet molding compound (SMC), plastics, and metals. It features a 1:1 by volume mix ratio and simplifies production by requiring only a dry wipe for surface preparation before bonding.

Key features

  • Fast fixture time: Achieves handling strength in just one minute on a heated fixture at 240°F (116°C).
  • Minimal surface preparation: Eliminates complex pre-treatment steps by requiring only a simple dry wipe prior to application.
  • Reliable performance: Offers good flexibility, high sag resistance, and excellent heat resistance up to a 217°F (103°C) glass transition temperature.

Applications / Suitable for

  • Designed for bonding sheet molding compound (SMC).
  • Suitable for bonding various plastics and metals.
Product Family

HARDENER HV 8503

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
beige
Pot Life
30 minutes
Specific Gravity
1.21
Thermal Properties
Glass Transition Temperature (Tg)
103 °C
Mechanical Properties
Elongation
15 %
Physical Properties
Viscosity (Part B)
368000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Pre-cure processing characteristics and physical properties of Araldite® AV 8503 / HV 8503.

Property Value Unit Method / condition
Mix Ratio (Volume) 1:1 - Resin to Hardener
Mix Ratio (Weight) 100:92 - Resin to Hardener
Viscosity (Resin) 172,000 cP Brookfield @ 10 rpm, 77°F
Viscosity (Hardener) 368,000 cP Brookfield @ 10 rpm, 77°F
Pot Life 30 minutes at 77°F, 100g mass
Sag Resistance 0.08 (2) inch (mm) at 77°F (0.23 in/6mm bead)
Technical properties

After-processing / final-state properties

Cured mechanical properties of Araldite® AV 8503 / HV 8503 after full cure.

Property Value Unit Method / condition
Hardness 78 Shore D -
Ultimate Tensile Strength 3400 (23.4) psi (MPa) ASTM D-638
Elongation 15 % ASTM D-638
Lap Shear Strength (Aluminum) 3380 (23) psi (MPa) Cure: 1 hour at 250°F, tested at 77°F
Glass Transition Temperature 217 (103) °F (°C) -
Young's Modulus 142,000 (979) psi (MPa) ASTM D-638