FREKOTE WOLO

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

FREKOTE WOLO

Main features

  • Wipe Application Method
  • Mold Release and Sealing Capability
  • 15-Minute 20 deg C Cure

Product Description

LOCTITE® FREKOTE® WOLO is a clear, colorless, solvent-based polymeric mold release agent for fiberglass-reinforced plastic and polyester-resin molding. Its wipe-on-leave-on application forms a thin, uniform coating without a separate polishing step. The moisture-sensitive material cures at room temperature and provides a high-gloss finish with multiple releases and minimal mold buildup. Because the formulation includes mold-sealing capability, fully cured molds can be prepared without a separate sealer by applying the documented coating sequence. Initial application requires at least four coats, with five minutes between coats and a 15-minute final cure at 20°C.

Key features

  • Wipe-on-leave-on application: Applied with a lint-free cloth and left on the mold surface to evaporate and cure.
  • High-gloss finish: Produces a high-gloss finish on FRP polyester parts without a separate polishing step.
  • Integrated mold-sealing capability: Can seal fully cured molds when the documented additional-coat procedure is followed.
  • Fast room-temperature cure: Requires five minutes between coats and a 15-minute final-coat cure at 20°C.
  • Multiple-release performance: Supports multiple releases with minimal mold buildup under the recommended application conditions.

Applications / Suitable for

  • Fiberglass-reinforced plastic molds
  • Polyester-resin molding processes
  • High-gloss FRP polyester parts
  • Fully cured molds requiring combined sealing and release treatment
  • Touch-up of complete molds or localized high-wear areas
Product Family

FREKOTE WOLO

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Clear Liquid
Specific Gravity
0.71–0.73
Thermal Properties
Temperature Resistance
400 ˚C

Additional Information

Technical properties

As-supplied / before-processing properties

Documented as-supplied characteristics and application conditions for LOCTITE® FREKOTE® WOLO.

Property Value Unit Method / condition
Appearance Clear, colorless — As supplied; LMS-controlled characteristic
Chemical type Solvent-based polymer — Polymeric mold release liquid
Odor Hydrocarbon — As supplied
Specific gravity 0.71–0.73 — At 25°C; LMS-controlled characteristic
Cure mechanism Room-temperature, moisture cure — Applied release coating; product is moisture sensitive
Application temperature 13–41 °C Recommended mold-surface application range
Minimum time between coats 5 min Before application of the next coat
Final-coat cure time 15 min At 20°C after the initial minimum four-coat application
Optimal storage temperature 8–21 °C Unopened container in a dry location
Technical properties

After-processing / final-state properties

Documented characteristics of the applied and cured LOCTITE® FREKOTE® WOLO release coating.

Property Value Unit Method / condition
Finish reflection High gloss — FRP polyester molded-part finish; no separate polishing step required
Release behavior Multiple releases — Polyester resins under recommended preparation and application conditions
Mold buildup Minimal — Supplier-documented qualitative characteristic
Cured thermal stability ≤400 °C Cured release coating; not an application or continuous service-temperature rating