FREKOTE R-220

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

FREKOTE R220

Main features

  • High-Slip EPDM/Elastomer Release
  • 60 to 205 deg C Mold Operation
  • 4-Minute 149 deg C Cure

Product Description

LOCTITE® FREKOTE® R-220 is a one-part, water-based, heat-curing mold release emulsion for demanding rubber molding processes. Its high-slip characteristics make it particularly relevant for difficult-to-release materials such as EPDM and highly filled elastomers. Applied as a finely atomized spray to a preheated mold, the product chemically bonds to the surface and forms a thin, inert, thermally stable release coating. It also supports thermoplastic urethanes and solid polyurethane cast elastomers across mold application temperatures from 60°C to 205°C.

Key features

  • High-slip release performance: Formulated for difficult-to-release rubbers, including EPDM and highly filled elastomers.
  • Water-based formulation: Supplied as a non-flammable, milky-white emulsion with mild odor.
  • Heat-cured coating: Chemically bonds to preheated mold surfaces to form a thin, inert release layer.
  • Fast application and cure: Multiple coats can be applied to the heated mold, with full cure in 4 minutes at 149°C.
  • Gloss finish: Produces a gloss finish under the documented application conditions.

Applications / Suitable for

  • EPDM and other difficult-to-release rubber compounds
  • Highly filled elastomers
  • Thermoplastic urethanes
  • Solid polyurethane cast elastomers
  • Preheated molds operating from 60°C to 205°C
Product Family

FREKOTE R-220

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

General Properties
Color
Milky-white emulsion
Specific Gravity
0.95–1.06
Thermal Properties
Temperature Resistance
315 ˚C

Additional Information

Technical properties

As-supplied / before-processing properties

Documented as-supplied characteristics and application conditions for LOCTITE® FREKOTE® R-220.

Property Value Unit Method / condition
Appearance Milky-white emulsion — As supplied
Chemical type Water-based emulsion — One-part mold release agent
Odor Mild — As supplied
Specific gravity 0.95–1.06 — At 25°C; typical value range
pH 3.9–4.1 — Typical as-supplied value
Application temperature 60–205 °C Preheated mold surface
Full cure time 25 / 10 / 4 min At 60°C / 93°C / 149°C, respectively
Optimal storage temperature 8–21 °C Unopened container in a dry location
Technical properties

After-processing / final-state properties

Documented characteristics of the applied and heat-cured LOCTITE® FREKOTE® R-220 release coating.

Property Value Unit Method / condition
Cured thermal stability ≤315 °C Heat-cured release coating
Release-film form Thin, inert coating — Chemically bonded to a properly prepared, preheated mold surface
Finish reflection Gloss — Henkel product-page technical specification
Release behavior Multiple releases — Supplier-documented characteristic under recommended application conditions