FREKOTE R-120

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

FREKOTE R-120

Main features

  • Semi-Permanent Rubber-Mold Release Coating
  • 4-Minute 150 deg C Cure
  • Multiple Releases with Low Transfer

Product Description

LOCTITE® FREKOTE® R-120 is a one-part, water-based, semi-permanent release agent for rubber molding. Applied as a finely atomized spray to a preheated mold, it chemically bonds to the surface and forms a thin, inert, thermally stable release coating. The product supports natural and synthetic rubber polymers, including some thermoplastic urethanes, across mold application temperatures from 60°C to 200°C. It is intended for demanding molding processes where minimal mold buildup and low transfer to the molded part are required.

Key features

  • Water-based formulation: Supplied as a translucent, non-flammable emulsion with mild odor.
  • Semi-permanent release coating: Chemically bonds to a preheated mold surface to support multiple releases.
  • Broad application-temperature range: Suitable for mold temperatures from 60°C to 200°C.
  • Fast heat cure: Full cure time decreases as mold temperature increases, reaching 4 minutes at 150°C.
  • Controlled mold condition: Recommended where minimal mold buildup and low transfer to molded parts are required.

Applications / Suitable for

  • Natural and synthetic rubber molding
  • Some thermoplastic urethane molding applications
  • Demanding molding processes requiring minimal mold buildup
  • Preheated molds operating from 60°C to 200°C
Product Family

FREKOTE R-120

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Translucent emulsion
Specific Gravity
0.98–1.02
Thermal Properties
Temperature Resistance
315 ˚C

Additional Information

Technical properties

As-supplied / before-processing properties

Documented as-supplied characteristics and application conditions for LOCTITE® FREKOTE® R-120.

Property Value Unit Method / condition
Appearance Translucent emulsion — As supplied; LMS-controlled characteristic
Chemical type Water-based emulsion — One-part semi-permanent release agent
Odor Mild — As supplied
Specific gravity 0.98–1.02 — At 25°C
pH 3.9–4.1 — LMS-controlled characteristic
Application temperature 60–200 °C Preheated mold surface
Full cure time 25 / 10 / 4 min At 60°C / 93°C / 150°C, respectively
Optimal storage temperature 8–21 °C Unopened container in a dry location
Technical properties

After-processing / final-state properties

Documented characteristics of the heat-cured LOCTITE® FREKOTE® R-120 release coating.

Property Value Unit Method / condition
Cured thermal stability ≤315 °C Heat-cured release coating
Release-film form Thin, inert coating — Chemically bonded to a properly prepared, preheated mold surface
Epoxy release test ≥4 — LMS-controlled cured-material test
Finish reflection Matte — Henkel product-page technical specification