FREKOTE PUR-100

Harmonization Code : 3215.19 | Printing ink, excluding black ink, and includes solder masks

FREKOTE PUR-100

Main features

  • Water-Based Non-Flammable Release
  • Multiple Releases Per Application
  • Paint-Ready Molded Parts

Product Description

LOCTITE FREKOTE PUR-100 Mold Release Agent is a water-based heat-cure emulsion for releasing rigid high-density polyurethane foam, cast polyurethane parts, and some low-density polyurethane foams. The milky white product has a specific gravity of 0.97 to 1.03 and is non-flammable, freeze/thaw stable, low in VOC, and non-settling. It is spray applied to molds preheated to at least 60 deg C and is suitable for mold temperatures up to 200 deg C. The cured polymer film supports multiple releases and allows molded parts to be painted without post-finishing or cleaning.

Key features

  • Water-based non-flammable system: The release agent uses a water-based emulsion that is non-flammable and freeze/thaw stable.
  • Multiple-release polymer film: A single application can provide multiple releases under the documented molding conditions.
  • Post-molding paintability: Molded parts can be painted without post-finishing or cleaning.

Applications

  • Rigid high-density polyurethane foam molding
  • Cast polyurethane part release
  • Selected low-density polyurethane foam molding
Product Family

FREKOTE PUR-100

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Milky White Emulsion
Component System
Water Based Emulsion
Thermal Properties
Operating Temperature
>60 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid, storage, and mold-temperature data before formation of the release film.

Property Value Unit Method / condition
Appearance Milky white emulsion - As supplied
Chemical type Water-based emulsion - As supplied
Specific gravity 0.97 to 1.03 - At 25 deg C
Cure type Heat cure - Release coating
Minimum application temperature >= 60 deg C Apply to a preheated mold
Maximum mold temperature 200 deg C Suitable application limit
Recommended storage temperature 5 to 25 deg C Optimal unopened-container storage
Technical properties

After-processing / final-state properties

Cure schedule and applied-film performance for polyurethane molding.

Property Value Unit Method / condition
Full cure at 60 deg C 30 min After spray application
Full cure at 100 deg C 10 min After spray application
Full cure at 150 deg C 4 min After spray application
Minimum coating count 4 coats For molds at 60 to 120 deg C
Hot or porous mold coating count 6 coats For 120 to 200 deg C molds or porous molds
Release-cycle capability Multiple releases - From a single application under stated conditions
Post-molding finish Paintable without preparation - No post-finishing or cleaning required before painting