FREKOTE FMS

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

FREKOTE FMS

Main features

  • Composite-Mold Microporosity Sealing
  • High-Gloss Prepared Mold Surface
  • 20-Minute Final-Coat Cure at 20 deg C

Product Description

LOCTITE® FREKOTE® FMS is a clear, colorless, solvent-based polymeric mold sealer formulated for fiberglass-reinforced polyester, epoxy, and other composite molds. Applied by wiping during mold preparation, it seals microporosity and slight surface imperfections to create a uniform base for subsequent mold release-agent application. The room-temperature-curing sealer is particularly relevant for new or “green” molds and repaired areas, providing a high-gloss surface with straightforward application and a 20-minute final-coat cure at 20°C.

Key features

  • Composite mold sealing: Formulated for fiberglass-reinforced polyester, epoxy, and other composite molds.
  • Microporosity control: Seals microporosity and slight surface imperfections in new, green, or repaired molds.
  • High-gloss preparation: Produces a high-gloss mold surface and supports uniform release-agent application.
  • Wipe-on application: Applied using a clean, lint-free cotton cloth.
  • Fast room-temperature cure: Final coat cures in 20 minutes at 20°C.

Applications / Suitable for

  • Fiberglass-reinforced polyester molds
  • Epoxy and other composite molds
  • New or green molds with microporosity
  • Repaired mold surfaces and areas with slight imperfections
  • Mold preparation before applying a compatible release agent
Product Family

FREKOTE FMS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Clear Liquid
Specific Gravity
0.757–0.771

Additional Information

Technical properties

As-supplied / before-processing properties

Documented as-supplied characteristics and application conditions for LOCTITE® FREKOTE® FMS.

Property Value Unit Method / condition
Appearance Clear, colorless — As supplied; LMS-controlled characteristic
Chemical type Solvent-based polymer — As supplied
Odor Hydrocarbon — As supplied
Specific gravity 0.757–0.771 — At 25°C; LMS-controlled characteristic
Application temperature 13–35 °C Recommended application range
Minimum time between coats 15 min Before applying the next coat
Final-coat cure time 20 min At 20°C
Technical properties

After-processing / final-state properties

Documented characteristics of the prepared mold surface after application and curing.

Property Value Unit Method / condition
Surface finish High gloss — Cured mold-sealer surface
Surface-sealing function Seals microporosity and slight surface imperfections — New, green, or repaired composite molds
Release-system preparation Uniform release-agent coating — Prepared base surface before compatible release-agent application