FREKOTE 710-LV

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

FREKOTE 710-LV

Main features

  • Room-Temperature Semi-Permanent Release
  • High-Slip High-Gloss Finish
  • Controlled Two-Coat Application

Product Description

LOCTITE FREKOTE 710-LV Mold Release Agent is a solvent-based semi-permanent polymer mold release treatment for epoxies, thermosets and prepregs, polyester resins, thermoplastic compounds, and high-performance composites. The clear, colorless liquid has a specific gravity of 0.809 to 0.817 and is applied at 13 to 41 deg C. Two initial coats are used on cleaned, dry molds with 5 to 10 minutes between coats, followed by a 15 to 20 minute final cure at 25 deg C. The cured treatment provides a high-slip, high-gloss release surface with room-temperature cure.

Key features

  • Room-temperature semi-permanent release: The polymer treatment cures at room temperature to form a semi-permanent release surface.
  • High-slip high-gloss finish: The cured treatment is positioned for high slip and a high-gloss molded finish.
  • Controlled two-coat application: The initial mold treatment uses two coats with defined intercoat and final-cure times.

Applications

  • Release of epoxies, thermosets, and prepregs
  • Release of polyester resins and thermoplastic compounds
  • High-performance composite molding
Product Family

FREKOTE 710-LV

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Clear colorless liquid
Component System
Solvent Based Polymer
Thermal Properties
Operating Temperature
13 - 41 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid and application-range data before treatment of the mold surface.

Property Value Unit Method / condition
Appearance Clear, colorless liquid - As supplied
Chemical type Solvent-based polymer release agent - As supplied
Specific gravity 0.809 to 0.817 - Typical liquid value
Application temperature 13 to 41 deg C Mold and ambient application range
Recommended storage temperature 8 to 21 deg C Store in the recommended range
Technical properties

After-processing / final-state properties

stated applied-film characteristics and cure conditions for the treated mold surface.

Property Value Unit Method / condition
Release-film type Semi-permanent polymer treatment - After the stated coating and cure process
Initial coating sequence 2 coats Apply to a cleaned, dry mold
Intercoat time 5 to 10 min Between initial coats
Final cure 15 to 20 min At 25 deg C
Release characteristic High slip - Cured mold-release surface
Molded-surface finish High gloss - Release-finish characteristic