FCT NL930PT

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

FCT NL930PT

Main features

  • ROL0 Zero-Halide Flux
  • Eight-Hour Stencil Life
  • Multiple Lead-Free Alloy Options

Product Description

FCT NL930PT No-Clean Lead-Free Solder Paste is a no-clean lead-free solder paste with pin-testable flux residue for SMT printing and reflow. The flux system is classified ROL0 and is stated with 0.0% halide ion and halogen content. Available alloy options include SAC305, SN100C, Sn96.5/Ag3.5, SN100CV, LF-C2, and anti-tombstoning mixtures in supported powder sizes. The paste is formulated for fine-pitch and small-area-ratio apertures, provides an 8 hour stencil life under the stated temperature and humidity conditions, and supports reflow within approximately 8 hours after printing.

Key features

  • ROL0 zero-halide flux: The flux classification is ROL0 with 0.0% documented halide ion and halogen content.
  • Eight-hour stencil life: The paste maintains a documented stencil life under controlled temperature and humidity.
  • Multiple lead-free alloy options: Supported configurations include SAC305, SN100C, SN100CV, LF-C2, and Sn96.5/Ag3.5.

Applications

  • Lead-free no-clean SMT solder-paste printing and reflow
Product Family

FCT NL930PT

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

Other Properties
Stencil Life
8 hours

Additional Information

Technical properties

As-supplied / before-processing properties

Flux, alloy, powder, stencil-life, and handling data before reflow.

Property Value Unit Method / condition
Physical form Paste - As supplied
Flux classification ROL0 - J-STD-004B
Halide ion content 0.0 wt % IPC 2.3.28.1
Halogen content 0.0 wt % EN 14582 and IPC 2.3.28.1
Solder alloy options SAC305; SN100C; Sn96.5/Ag3.5; SN100CV; LF-C2; anti-tombstoning mixtures - Powder size varies by alloy and configuration
Solder powder types Type 3 or 4; Type 5 size range stated - Availability depends on alloy/configuration
Stencil life 8 h At 18 to 29 deg C and 10 to 70% RH
Warm-up time 3 to 4 h Sealed container to 18 to 29 deg C before use
Printed-board hold time Approximately 8 h Reflow as soon as practical after printing